Landfill Geomembrane with Smooth Surface
- Loading Port:
- China Main Port
- Payment Terms:
- TT OR LC
- Min Order Qty:
- -
- Supply Capability:
- -
OKorder Service Pledge
OKorder Financial Service
You Might Also Like
1. Geomembrane specifications
1) Thickness : 0.15mm - 4.0mm.
2) Width : Within 8 m (1m-8m).
3) Length : 50m-100m/roll (as request).
4) Material : HDPE,( LDPE, LLDPE, PVC, EVA ).
5) Color : Black , white , red , blue , or as required.
6) Optional surface : Textued(one or two side) or smooth surface.
7) Certificate:CE/ISO9001,14001
2. HDPE geomenbrane Features
Good mechanical properties, high tear strength, deformation and adaptable, puncture resistance, anti-aging, anti-ultraviolet-resistant, Anti oil and salt, pH, anti-corrosion, high temperature-resistant, non-toxic, long service life. water, drainage, seepage, the good effect of moisture, width, thickness of the full range of specifications and low cost, simple construction.
No. | Item | Test Value | ||||||
0.75mm | 1.0 mm | 1.25 mm | 1.5 mm | 2.0 mm | 2.5 mm | 3.0mm | ||
1 | Minimum Density(g/cm³) | 0.939 | ||||||
2
| Tensile Property | |||||||
Strength at yield,N/mm | 11 | 15 | 18 | 22 | 29 | 37 | 44 | |
Strength at break ,N/mm | 20 | 27 | 33 | 40 | 53 | 67 | 80 | |
Elongation at yield,% | 12 | |||||||
Elongation at break,% | 700 | |||||||
3 | Tear Resistance N | 93 | 125 | 156 | 187 | 249 | 311 | 374 |
4 | Puncture Resistance N | 240 | 320 | 400 | 480 | 640 | 800 | 960 |
5 | Stress Crack Resistance, hrs | 300 | ||||||
6 | Carbon Black Content, % | 2.0-3.0 | ||||||
Carbon Black Dispersion | 1 or 2 | |||||||
7 | Standard OTI Min | 100 | ||||||
High Pressure OTI Min | 400 | |||||||
8 | Impact Cold Crack at -70°C | Pass | ||||||
9 | Water vapor permeability (g.cm/cm2 .s.Pa) | ≤1.0×10-13 | ||||||
10 | Dimensional Stability (%) | ±2 |
3. HDPE Geomembrane Applications
1) Environmental protection, sanitation (such as solid waste landfills, sewage treatment plants, power plants Chi-conditioning, industrial, hospital solid waste, etc.) .
2) Water (such as rivers, lakes and reservoirs of the anti-dam, plugging, reinforcement of the canal seepage, the vertical wall of the heart, slope protection, etc.).
3) Municipal Engineering (subway, on the ground floor of the building, planted roof, the roof garden of anti-seepage, sewage pipes lining, etc.).
4) Landscape (man-made lake, river, reservoir, golf courses reservoirs of the substrate, slope protection, green lawn of the waterproof moisture, etc.).
5) Petrochemical (chemical plants, oil refineries, gas storage tanks of the anti-chemical reaction tanks, sedimentation tanks of the lining, etc.).
6) Mining (washing and pool heap leaching, the ash-field, dissolved, precipitation, the yard, the tailings seepage substrates, etc.) .
- Q: Foam concrete for the roof cushion generally do much bulk ah
- in recent years, the density of 160kg / m3 ultra-light foam concrete is also used in construction projects.
- Q: When the cushion is used, the thickness of the protective layer is not less than ()
- Basement roof: non-load protection layer generally use C20 fine stone concrete or reinforced concrete, the thickness of 50 ~ 80mm. The road, driving the protective layer is determined by design.
- Q: Why do the basics of the cushion waterproofing
- Raft foundation do not do waterproof mainly depends on the design of the groundwater level considerations, calculated if the floor itself to meet the requirements, you can not do, and not rigid to do
- Q: The top floor made waterproof playing cushion layer of how to do
- Roof waterproofing can not use a single waterproof material, must be rigid and flexible combination of construction, flexible waterproof stretch is good, a little bit of settlement or deformation will not damage the waterproof layer. Rigid waterproof (ie mortar waterproofing agent) waterproof at the same time, can play a protective role, waterproof layer is not easy to be destroyed.
- Q: The roof cushion is waterproof on the slope roof
- Most of the slope roof itself is not waterproof. The role of the slope roof is used for drainage,
- Q: Is the raft cushion waterproofing full of the cushion?
- The request is full. Raft foundation do not do waterproof mainly depends on the design of the groundwater level considerations, calculated if the floor itself to meet the requirements, you can not do, and not rigid to do.
- Q: Can the floor tiles be removed from the cement mats on the prefabricated board floor?
- You can dig, but be careful not to use a strong earthquake with the machinery to remove, otherwise it will damage the original structure.
- Q: What is the difference between leveling and cushion?
- Commonly used materials are, cement mortar leveling layer, fine stone concrete leveling layer, asphalt mortar leveling layer and so on. Leveling layer and the difference between the cushion, which is a very easy to confuse the two engineering concepts.
- Q: How to build a fine stone concrete cushion?
- The cushion is primarily responsible for the load coming from the surface and passes the load evenly to the structural or base.
- Q: Basement floor mattress dry to what degree can do coil waterproof?
- First, the basement moisture treatment structure is usually: first in the basement wall outer surface wiping 20mm thick 1: 2 waterproof mortar, basement walls should be used cement mortar masonry, gray seam must be full; and in the basement floor and the first Floor floor is divided into two walls of the level of moisture-proof layer. The outer wall of the basement wall should be tampered with the soil with poor permeability.
Send your message to us
Landfill Geomembrane with Smooth Surface
- Loading Port:
- China Main Port
- Payment Terms:
- TT OR LC
- Min Order Qty:
- -
- Supply Capability:
- -
OKorder Service Pledge
OKorder Financial Service
Similar products
Hot products
Hot Searches
Related keywords