• Laminate Flooring 8mm Export to Europe 7-12mm Double Click System 1
  • Laminate Flooring 8mm Export to Europe 7-12mm Double Click System 2
  • Laminate Flooring 8mm Export to Europe 7-12mm Double Click System 3
  • Laminate Flooring 8mm Export to Europe 7-12mm Double Click System 4
Laminate Flooring 8mm Export to Europe 7-12mm Double Click

Laminate Flooring 8mm Export to Europe 7-12mm Double Click

Ref Price:
get latest price
Loading Port:
Shanghai
Payment Terms:
TT OR LC
Min Order Qty:
2000 m²
Supply Capability:
2000000 m²/month

Add to My Favorites

Follow us:


OKorder Service Pledge

Quality Product, Order Online Tracking, Timely Delivery

OKorder Financial Service

Credit Rating, Credit Services, Credit Purchasing

Introduction:

Laminate flooring is a multi-layer synthetic flooring product, fused together with a laminationprocess. Laminate flooring ismost often four layers of materialsFrom topto bottom is Durable Overlay, Decorative Paper, HDF board, Balance Paper.

Durable Overlay is made by applying an AL2O3 solution over transparent paper, AL2O3 is very fineand thus it does not hide the color and design of the decorative paper.

Decorative Paperis a computer made paper which imitates natural wood, stone etc, by applying AL2O3to decorative paper, the latter becomes protected from the environment.

HDF board are made of wood fiber compressed into a high density panel (≥880kgs/m3).

Balance Paper is the thick and strong paper treated with AL2O3 on the back of laminate flooring,it gives stability to the laminate flooring boards and provide a measure ofisolation from under-floor humidity.

Wear Rating:

Durable Overlay Thickness

Applying Place

Euro Grade

EN438

EN13329

China National Stand

22gm2

21 Family Low Grade

AC1

2000

≥600

1500

33gm2

22 Family Medium Grade

AC2

4000

≥900

2500

39gm2

23 Family High Grade

AC3

6000

≥1800

4000

45gm2

31 Commercial Low Grade

AC3

9000

≥2500

6000

62gm2

32 Commercial Medium Grade

AC4

12000

≥4000

9000

76gm2

33 Commercial High Grade

AC5

15000

≥6500

12000

Formaldehyde EmissionE1

Moisture Content≤12%

Surface: Mirror, Middle Emboss, Fine Emboss, Crystal, Hand Scraped        

Specification:

Thickness: 7.3mm,8.3mm, 12.3mm, 15.3mm

Based on order, other specification are alsoavailable.

Packing: 8-10 pieces per carton, 35-60 cartons perpallet, about 20 pallets per container.

 Laminate Flooring 8mm Export to Europe 7-12mm Double Click

Q:How thick is the composite floor?
The thickness of the composite floor is 1.5, and the number is higher or less than this number is not standard. Registered trademark, production date, serial number or batch number, formaldehyde emission, wear-resistant value of these are more must have, generally good middle of the composite floor layer should be Liuhe wood, this is the middle of the composite floor soft Coefficient parameters larger, not easy to deformation!
Q:How to check the composite wood floor shop is good
The appearance of flat, step on the real, close side of the beautiful.
Q:100 locusts know Hao version of Tongbao Kun ready to buy wood flooring, a friend said that the composite floor of the radiation formaldehyde or something. Answer, the composite wood floor with radiation and formaldehyde? How to identify and buy more environmentally friendly wood flooring more
Home furnishings or 100 locusts know Hao version of Tongbao Kun with solid wood flooring, or with tiles. Composite wood flooring is a commercial, the indoor air dip or more serious. Pollution mainly from the floor of the adhesive in the benzene compounds, the human organs caused irreversible damage. Formaldehyde harm is very small, only 10% of the total pollution is less than.
Q:Just renovated soon, the bottom of the plumbing. Now the corner of the solid wood composite floor darkened, and little by little bigger. It is water and water leakage, but the pressure of the boiler has not changed.
It should be said that your water pipe is leaking, the wood flooring absorbs the color after dark, more important is that your wooden floor and water swelling, so you see is little by little bigger, indicating that the leakage is very small , So you feel the pressure of the furnace did not change, as soon as possible to remove the wood flooring at the inspection of the water pipe, I judge the torture will be a trace of the pile of pepper standard bowl of water is a trachea, must be resolved soon ah.
Q:Any suggestions for care and cleaning of a new engineered floor?
Follow the instructions given by whoever laid it.
Q:The composite floor is a good reason to use a straight pavement or a keel
The ground leveling; remember to stay the thickness, usually about 1.7, and then paved before the clean-up, the ground clean up, put the floor under the moisture-proof pad, tasting taste of enlightenment to Germany to avoid the spring glass do not take tin foil, airtight is also easy to distribute heavy metals , The general composite flooring are straight shop, that is, do not play keel, do not fight nails, if the keel is more trouble, disassembly is also troublesome. Buy the floor, to build nest building materials to see home, Sihetadi floor style, affordable. The main products of home building materials are purchased directly from many of the top manufacturers of developed countries such as Germany, Italy, Netherlands, Belgium, Spain, France, USA, Japan and Korea. Domestic products are also from the international standards of export-oriented enterprises direct procurement. All product quality is in line with the European Union, the United States, China or other world-class international certification standards. Nest a professional international procurement team, each year around the world of professional building materials home exhibition, visit thousands of professional manufacturers, carefully selected for each product.
Q:Lacquered floor and composite floor how to distinguish
Almost ~
Q:Please tell me that the Kelly floor is good
You see is the Kelly composite floor is it? Actually I tell you. Composite floor is not complicated to say that the simple point is the grass-roots "is the floor density board" wear surface "surface wear speed" environmental protection rate of these three aspects to proceed like a composite wood flooring do not need to pay too much attention to brand identification way to tell you To a product model you like to return home, find a little bit of the fish tank with water and goldfish to measure the thickness of the sample, such as your choice is 1.2 thickness of the wooden floor you good, and then put your sample Fish tank, 24 hours after you take out the sample to see the thickness as long as 1.2 or no more than 1.22 to 1.23 is the density and water swelling coefficient qualified, and then look at the water mixture and the fish is dead, if the fish are all right to prove Environmental protection qualified for you and your family will not receive decoration pollution. With the gauze 360 ??purpose not too thick "Building Materials City have sold a good quality gauze 360, such as sharp card 0.6 a" hard to polish your hands in the sample surface if repeated polished 10 times no times raft Rubbing the right to protect the problem to prove that the number of wear and tear to reach the standard. Finally, we must keep the sample, when buying goods to see the goods to prevent you to change. These are the choice of composite floor of some of the methods, I hope you from the elephant elephant Euclide Kelly Hongji up hamburger and other brands of the floor to choose your favorite and qualified composite floor hope LZ adoption Thank you
Q:Multi-layer parquet, for geothermal, when the shop to shop moisture-proof pad? why? Do you want to play keel?
Multilayer solid wood flooring installation whether to play keel, depending on their own circumstances. General multi-layer solid wood flooring playing keel, the foot feeling comfortable, more durable. But the cost of multi-layer solid wood flooring keel than other installation methods to be more expensive. First, the multi-layer solid wood flooring construction preparatory work: 1, the floor construction must be arranged at the end of all the decoration, in order to avoid other construction damage paint; 2, pavement floor must be dry, smooth; 3, Sprinkle a layer of mothproof powder. Second, the multi-layer solid wood flooring installation method: 1, straight paste method: like solid wood flooring installation, playing keel pavement; 2, straight shop method: the use of composite flooring method (that is, directly on the ground pavement); 3, high law: first on the ground covered with 62.5px thick pavement treasure. And then shop the moisture pad, and finally covered with multi-layer solid wood flooring.

1. Manufacturer Overview

Location
Year Established
Annual Output Value
Main Markets
Company Certifications

2. Manufacturer Certificates

a) Certification Name  
Range  
Reference  
Validity Period  

3. Manufacturer Capability

a)Trade Capacity  
Nearest Port
Export Percentage
No.of Employees in Trade Department
Language Spoken:
b)Factory Information  
Factory Size:
No. of Production Lines
Contract Manufacturing
Product Price Range

Send your message to us

This is not what you are looking for? Post Buying Request

Similar products

Hot products


Hot Searches

Related keywords