Eco Freindly Wood Plastic Composite Decking
- Loading Port:
- Shanghai
- Payment Terms:
- TT OR LC
- Min Order Qty:
- 500 m²
- Supply Capability:
- 10000 m²/month
OKorder Service Pledge
OKorder Financial Service
You Might Also Like
Specification
Packaging & Delivery
Packaging Detail: | Packed with pallet. |
Delivery Detail: | Within 2 weeks got the deposit. |
Specifications
wpc decking
1.Place of Origin: CN; ZHE;
2.Features: Waterproof,Fireproof;
3.Application:park,garden.
4.Certificate: ISO 9001
Product Description
2014 New Outdoor 146x24mm WPC Decking Prices For Public
Wood plastic composite(WPC)made of 50% wood fiber and 50% PP,PE or PVC resin together with specialized ingredients, imported pigment, and anti-UV material. WPC products possess the advantages of good intensity, high rigidity, durable usage period, moisture proof, anti-abrasion, heat insulation, fire-resistant, aging-resistant, cauterization-resistant, water proof, insect resistant, and no painting needed. WPC products can be widely used in public garden or park, construction decoration, villa garden and so on.
Features:
(1) Insect-proof
(2) Durable, economic.
(3) Cost low in maintenance.
(4) Brand range of appearance and color.
(5) Environmentally friendly, recyclable.
(6) Looks and feels like nature wood.
(7) Easily and conveniently installed and cleaned.
(8)Stable over a wide temperature range, weather resistant,especially can be used in the open air.
Technical Index:
Techinical Index | |||
No. | Property | Result | Text Method |
1 | Density | 1.23g/cm | ASTMD792 |
2 | Water absorption | 0.50% | ASTMD570-00 |
3 | Tensile strength | 14.2Mpa | ASTMD638-03 |
4 | Elongation Rate at break | 3.90% | ASTMD638-03 |
5 | Flexural strength | 30.0Mpa | ASTMD790-03 |
6 | Flexural modulous | 3500Mpa | ASTMD790-03 |
7 | Linear expansibility | 4.9×10—5°C-1 | ASTMD696-03 |
8 | Compress strength | 26.4 | ASTM695-02 |
9 | Impact streght(unnotched)-25°C—+30°C | 90.1 J/m | ASTMD256-03 |
FAQ:
1.Price Term:FOB,CFR,CIF.
2.Port of Loading:Shanghai.
3.Payment Term:30% T/T in advance,70% balance against B/L copy.
4.Delivery Time:7-10 days after receiving your deposit for one 20 feet container.
- Q: I said he did not leveling the ground, obviously there is a place to step up to subsidence, he said the floor he was leveling, and to the floor, he said, Sinking is because the paved film, the membrane interface edge helium helpless Jurassic rhinoceros rhinoceros baskets will certainly be uneven, so will go subsidence! I would like to ask, he is not in the nonsense! Question added: decoration master began playing edge Helium dare to teach the gnome insects rhinoceros baskets rogue ~ I want him to re-leveling his life and death refused ~ would like to ask if this is a good floor and then I covered with carpet sound can cover more
- Is completely in the nonsense, the ground is not flat, the floor on the edge of the helium helpless Juria insects rhinoceros will be stepped up and down flick, that there is a gap between the floor and the ground, the ground leveling did not do well, the floor will cause a lock Buckle bite at the friction, it will sound. So still rework it.
- Q: Cheap point of the composite floor how much money a square meter
- Composite floor cheaper to the ten to one hundred have, it is important to look at the quality, buy the floor of the skills: a look: high-quality composite floor surface smooth, gorgeous natural color, variety, complete specifications, the negative moisture balance layer thickness; Poor composite flooring surface rough, dark color, variety, specifications, single, negative moisture balance layer thin. Second, listen to: high-quality composite flooring and other hard objects with the time, issued a crisp and bright metal sound, and no obvious scratches; poor composite flooring with a key and other hard time, issued a dumb sound, and there are obvious scratches The The thickness of the composite floor size is the same, two pieces of floor splicing seamless, hand touch joints are very smooth; poor quality composite floor size varies, two pieces of floor splicing There is a clear gap, hand touch joints have a clear sense of concavity. Four smell: As the selection of materials and equipment is not the same, high-quality composite floor environmental pollution-free, rich natural flavor; low-quality composite floor essence is not obvious, and some even contain harmful chemical composition, emitting a pungent smell. Five asked: the production of high-quality composite flooring enterprises are larger scale, the manufacturer's address, telephone number marked very clearly, after-sales service is perfect, the product of the "Three Guarantees"; low-quality composite floor is not "three packs."
- Q: Home improvement with a good floor or a good tiles
- If the geothermal words, it is recommended to have tiles, not geothermal, then the floor will be better, because you can cool
- Q: How does the composite wood floor rise?
- Folded and renewed
- Q: I am buying 1/2 engineering flooring and I am going to put it down as a floating floor on a crawl space. My question is do I have to put down any moisture barrier or foam underneath?
- If the crawl space has a vapor barrier either on the ground or to the bottom of the joists, which is should, then just a standard foam type under layment is all thats needed. If no vapor barrier is on the under side of the joists you should put it on to protect the joists from moisture. Putting any vapor barrier on the flooring inside will protect the engineered floor but not protect the joists. You need the foam type under layment to allow the flooring to expend and contract normally. If you were to nail or staple the wood down then you would need felt or a rosin paper to help keep the wood quiet from wood to wood contact. Any questions you can email me through my avatar. GL
- Q: Can the floor be re-installed?
- Demolition can be demolished, but the general composite floor of the buckle is relatively soft, if the removal of accidentally damaged the buckle when the floor on the waste. If there is no glue before the installation, then the re-laying will not have an impact on the floor, there may be damaged only around the foot line, the cost of the foot line is the material and feet and re-lay the floor of the labor costs; Previously installed in the sizing, then the floor after the demolition can easily lead to damage (mainly around the floor of the tongue and groove due to the glue caused by the damage), and after the demolition of the floor to be treated with the tongue and groove, if the technology is not auxiliary Violation of China and the end of the ancient house or the degree of patience is not enough, will re-lay the old floor joints are not in place, affecting the quality and beauty
- Q: Just renovated soon, the bottom of the plumbing. Now the corner of the solid wood composite floor darkened, and little by little bigger. It is water and water leakage, but the pressure of the boiler has not changed.
- It should be said that your water pipe is leaking, the wood flooring absorbs the color after dark, more important is that your wooden floor and water swelling, so you see is little by little bigger, indicating that the leakage is very small , So you feel the pressure of the furnace did not change, as soon as possible to remove the wood flooring at the inspection of the water pipe, I judge the torture will be a trace of the pile of pepper standard bowl of water is a trachea, must be resolved soon ah.
- Q: Composite flooring installation requires tools,
- There are some fixed-floor installation tools are fixed, some are in accordance with their own installation techniques to their own custom, the installation of the master can buy some of the most basic installation tools such as circular saw, hammer, angle grinder, curve saw, straight Ruler, tape, woodworking saws, carpentry chisel, small hammer, angle ruler, ruler, pencil, special wood wedge, special wood, special retractor and floor glue. These are the tools to be prepared to lay the floor, the first floor of the floor moisture-proof plastic film, and then in the moisture-proof film on the floor, intestinal plaque prostitutes illusion to do Wei-wei and then use the nails to the corner of the skirt, moisture film, steel Nails, laying mats, corners. Pave the floor of the tools are generally self-made, there is no standard, you can do a Z-type tool, hold down with a hammer can knock on the other side can go. Mainly the scale of the gap to grasp, according to the home of the humidity and regional preparation, or later easy to drum from what.
- Q: I bubble two different brands of composite flooring, soak a night, its edge has a centimeter width of the bubble up, come up with drying, there is a piece of recovery to the original state, there is a piece has been restored, ask you master, Is all the laminate flooring will be the case, or that the two floors are not good, like the kind of big brand of water soaked after the water will not appear such a situation, there is no one tested ah? Please test friends Recommend a few shocks Museum can be Jiu Jiu turtle snow you feel good after the test brand. Thank you! More
- I suggest you go to the decoration of the real estate community to ask
- Q: Rhine sun composite floor how?
- Rhine sun flooring is Germany's Kono Group's wholly-owned enterprises in China, the main production EO-level floor, its environmental rating in the industry ahead.
Send your message to us
Eco Freindly Wood Plastic Composite Decking
- Loading Port:
- Shanghai
- Payment Terms:
- TT OR LC
- Min Order Qty:
- 500 m²
- Supply Capability:
- 10000 m²/month
OKorder Service Pledge
OKorder Financial Service
Similar products
Hot products
Hot Searches