Ductile Iron Pipe Fittings Made in China is Hot Sale
- Loading Port:
- Tianjin
- Payment Terms:
- TT OR LC
- Min Order Qty:
- 1 m.t.
- Supply Capability:
- 100 m.t./month
OKorder Service Pledge
OKorder Financial Service
You Might Also Like
1.Packaging & Delivery
Packaging Detail: | DN80-300 bundled with steel belt ( the bundle size see the product detail part) DN400-1200 are in bulk |
Delivery Detail: | at least 5days for MOQ |
2.Specifications
Ductile iron pipe comply with ISO2531/EN545
1)We are factory
2)Best quality
3)Competive price
4)On time delivery
3.Features:
Facilitating high resistance to loadings, pressure and vacuum with high tensile strength,
Enabling high resistance to corrosion,
Not requiring cathodic protection,
Less operating cost since cast pipes have larger nominal diameter than polyethylene pipes.
Being the best pipe in case of an earthquake, with its ability of resilience and resistance to impacts without deformation,
Long product life, exceeding 50 years,
Preserving the quality of water with healthy interior coating.
4.Applied Standards:
General Design | ISO 2531 |
Internal Lining | ISO 4179 |
External Coating | ISO 8179 |
Polyethylene Coating (Optional) | ISO 8180 |
5.Joint Types:
Push-on Type | TYT Type |
Standard Type |
6. Diameters:
Pipes | Ø80 – Ø1200 mm (L = 6m, and 5.7m) |
Fittings | Ø80 - Ø2200 mm |
7. Wall Thickness:
Pipes | C and K classes |
Fittings | Class K10 - K12 |
8.Test Pressures:
Pipes | for Ø80 - Ø300 mm | 50 bar / 40 bar |
for Ø350 - Ø600 mm | 40 bar / 30 bar | |
for Ø700 - Ø1000 mm | 32 bar / 25 bar | |
for Ø1100 - Ø2600 mm | 25 bar |
Fittings | for Ø40 - Ø300 mm | 25 bar (*) |
for Ø350 - Ø600 mm | 16 bar | |
for Ø700 - Ø2600 mm | 10 bar | |
(*16 bar for fittings with PN10 flanges) |
9.Materials:
Pipe | Ductile iron casting, minimum 420 MPa tensile strength |
Internal Lining | Concrete Lining, ISO 4179 |
Socket Internal 10.Lining | 200 micron epoxy coating |
External Coating | 70 micron bitumen coating on 130 gr/m2 zinc coating, ISO 8179 |
Fittings | Ductile iron casting, minimum 420 MPa tensile strength |
Internal Lining | Concrete Lining, ISO 4179 |
External Coating | 70 micron bitumen coating on 130 gr/m2 zinc coating, ISO 8179 |
- Q: I would like home made recipe for cleaning my clothes iron!
- In your glove box, under the piles of kleenex and other junk, are the books you got for the dealership. Among those small books will be one which containg the separate tire warranty provided by the tire manufacturerread it. Talk to the dealership and see if they can do something. The issue may not be in the tire, but in the rim. If it is the rim, the dealership and manufacturer are responsible. If it is the tire, then you may have a claim against the tire manufacturer. btw, toss that half eaten Snickers bar, it's only gonna melt and make a mess in the glove box.
- Q: Water that has trickled through copper bearing ore will have the characteristic color of copper solutions. One method used to recover the copper dissolved in such streams is to place scrap iron in wide shallow sections of the stream. See if you can design an experiment to recover the remaining copper left in the copper chloride solution from this experiment.I don‘t understand this. Why is scrap iron used. How and what experiment am I supposed to come up with
- Iron is more reactive than copper, so it will displace copper from solution. (The iron dissolves into the solution, and the copper precipitates out.) You could try plain steel wool (without built-in soap) as a source of the iron for this experiment. It has lots of surface area, so the iron will react more quickly than, say, the iron in a nail.
- Q: my friend just me they have 90% iron is this true?ps i have a low white blood count and i think i have low iron and need iron [
- A low white blood count is NOTHING that you can do about. It has to do with your body being able to fight off infection which is different than the red blood cells. The iron that is in different foods is to help build your iron for the red blood count, NOT white blood count. There is NO way to build up the white blood cells!!! You can only monitor white blood cells on a regular basis with your physician.
- Q: Where to getcheap iron sets? also
- Irons that are used for controlled hits like wedgesputterss. etc. need stiffer shafts. Long drive irons need a whip effect to get distance. You can get inexpensive irons (cheap) at golf stores, golf pro shops and prbably on line. These can be either second hand or knock offs on sale. Spartawo.
- Q: I spend alot of time golfing, and am looking around for a new set of irons. . What irons would you suggest and why?
- try out all the brands and which ever brands feels the best just go with that one. i tried out six drivers at golfsmith and several woods for a demo and to me the G-10 Driver was light weight and had a good feel.
- Q: any pictures of atomic orbital model for IRON?
- No, elemental iron is Fe. But iron (III) oxide is Fe2O3, not FeO3! So the equation so far should be: Fe + O2 --- Fe2O3 But then you have to balance the equation so that there's the same number of irons and oxygens on each side. So you have: 4 Fe + 3 O2 --- 2 Fe2O3
- Q: I hear that meteors that hit the earth have lots of iron.and the ancient people used that iron first, when creating stuff.So the moon must have lots of hits.does it have lots of iron on it?
- I forget the specifics, but only a small fraction of meteoroids are iron. It is believed that most of the iron in the prototype Earth/Moon stayed with the Earth after the two bodies separated. That is why the Earth is about 66% more dense than the moon. The amount of iron the moon collects from meteor strikes would be a tiny fraction of what the Earth has in its interior.
Send your message to us
Ductile Iron Pipe Fittings Made in China is Hot Sale
- Loading Port:
- Tianjin
- Payment Terms:
- TT OR LC
- Min Order Qty:
- 1 m.t.
- Supply Capability:
- 100 m.t./month
OKorder Service Pledge
OKorder Financial Service
Similar products
Hot products
Hot Searches
Related keywords