• Wire Braided Hydraulic Hose SAE 100R2AT System 1
  • Wire Braided Hydraulic Hose SAE 100R2AT System 2
  • Wire Braided Hydraulic Hose SAE 100R2AT System 3
Wire Braided Hydraulic Hose SAE 100R2AT

Wire Braided Hydraulic Hose SAE 100R2AT

Ref Price:
get latest price
Loading Port:
China Main Port
Payment Terms:
TT OR LC
Min Order Qty:
-
Supply Capability:
-

Add to My Favorites

Follow us:


OKorder Service Pledge

Quality Product, Order Online Tracking, Timely Delivery

OKorder Financial Service

Credit Rating, Credit Services, Credit Purchasing

SAE 100R2AT 2-wire braided hydraulic hosemade with oil and weather proof rubber, is both soft and portable. Withsynthetic rubber, the inner tube is air and oil proof. Also, in addition to oiland weather resistance, the rubber cover features superior abrasion and agingresistance

Parameter

Nominal Diameter

Inside Diameter

Reinforcement Diameter

Outside Diameter

Working pressure

Proof pressure

Burst pressure

Bend Radius

Weight

inch

mm

mm

mm

mm

bar

psi

bar

bar

mm

kgs/m

3/16

-3

4.6-5.4

10.6-11.7

13.3-14.1

350

5075

700

1400

100

0.25

1/4

-4

6.2-7.0

12.5-13.1

14.4-15.2

350

5075

700

1400

100

0.3

5/16

-5

7.7-8.5

14.2-14.8

16.3-17.1

297

4307

594

1188

115

0.36

3/8

-6

9.3-10.1

16.2~16.8

18.3-19.1

280

4060

560

1120

130

0.49

1/2

-8

12.3-13.5

19.4~20.0

21.5-22.3

245

3553

490

980

180

0.56

5/8

-10

15.5-16.7

22.8~23.4

25.0-25.8

192

2784

384

768

200

0.6

3/4

-12

18.6-19.8

26.4~27.2

28.6-29.4

157

2277

314

628

240

0.83

1

-16

25.0-26.4

33.9~34.7

36.3-37.1

140

2030

280

560

300

1.22

1-1/4

-20

31.4-33.0

42.8~43.6

45.3-46.1

113

1639

226

452

420

1.91

1-1/2

-24

37.7-39.3

49.2~50.0

51.7-52.5

87

1262

174

348

500

2.17

2

-32

50.4-52.0

61.9~62.7

64.4-65.2

78

1131

156

312

630

2.74



Q: How to make a rubber tube requires flow
Rubber pipes are made of high pressure rubber hose and low pressure rubber hose.Low pressure rubber hose is made of inner rubber, cloth, winding (cloth, winding layer number), outer rubber. High temperature processing and vulcanization.
Q: Why does Br2 corrode rubber tubes?
Br2 bromine gasBr2 bromine element at room temperature is dark brown liquid, soluble in water, 100g water can dissolve about 3G bromine. Highly volatile, toxic, steam strongly stimulate the eyes, mucous membranes and so on. The water solution is called bromine.
Q: What's the detailed size of hose connection for shower?
Hot and cold bath: take a bath with hot water before going to bed every day. The temperature of the water is within the limits of the body's tolerance. After washing, sleep in hot water for 15 minutes. After bathing was out of a sweat, after 3~4 minutes, and then into a basin of cold water or cold shower. Note that the hot and cold bath must be "hot before cold."".
Q: The basic buret is a rubber tube is inlaid with a glass bead to replace glass piston. Why this burets cannot be used to install Potassium Permanganate solution?
The rubber tube can be Potassium Permanganate oxidation
Q: My company does high-quality rubber tube, all of the core method, and why use EPDM to do the inner tube, it is difficult to take off the core, please point out! What's the reason?
The core needs to be removed, and if it is too long, the mandrel can be divided into two sections and separated from the 2 sides
Q: How to detect the reliability of rubber hose
Bending test: after bending the hose to a certain extent, measure the minimum outside diameter of the bending part and the ratio of the outside diameter before bending, the passing capacity of the steel ball and the bending force when the tube is pressurized.
Q: What are the properties of an oil resistant rubber hose?
The early detection of the hose can effectively prevent the hose from the quality problems caused by security risks, the people's production and life plays a necessary role in supervision and protection. One-stop provides the physical and chemical properties of product materials, reliability testing, safety assessment and component analysis, to achieve a full range of testing and protection, is an important basis for ensuring product operation!
Q: How to determine the tensile strength of GB rubber joint?
In the middle of the specimen, 4 parallel lines marked by the mark mark are used to mark two distances equal to the standard distance (type 1 is 25mm, type 2 is 20mm, and type 3 is lOmm), and each reticle shall be equidistant from the center of the sample. If the non-contact deformation measuring device is used, the proper marking device shall be used, and two parallel markings shall be placed on the narrow parallel part of the sample. Each mark shall be equidistant from the specimen center and perpendicular to the long axis of the specimen, and the specimen shall not deform during the marking.Style cutting, punching machine blanking note the above points, is to test the tensile strength of rubber joints based on, but also guarantee.
Q: What's the rubber sleeve of the expander?
Rubber joint called flexible rubber joint, soft rubber joints, rubber flexible joint, flexible joint, shock absorber, shock absorber, shock absorber pipe throat, is a kind of high elasticity, high air tightness, pipe joint resistance to medium and climate. The product uses rubber elasticity, high air tightness, medium resistance, weather resistance and radiation resistance etc., using polyester cord fabric skew high strength, strong stability and the hot and cold composite, after high pressure, mold temperature and curing.
Q: How much is a gas hose a metre? At least 1 meters, 5 safe?
1, liquefied petroleum gas will soften the ordinary rubber tube, please use special rubber tube.2, often check and clean hose, found aging, cracking, burn, rat worm bite marks, should be replaced immediately. It is recommended that the hose be replaced in two years under normal conditions.3, gas hose length of not more than 2 meters, after passing the place is not allowed to have electrical appliances.4, hose do not close to the stove surface, so as not to be flame barbecue.5, the hose does not cross the wall, doors and windows.6, do not press or fold the hose, so as not to plug, affecting the continuous gas supply.At the interface, and appliance, 7 hose valve, please use the pipe truss, to prevent the shedding of leakage.

Send your message to us

This is not what you are looking for? Post Buying Request

Similar products

Hot products


Hot Searches

Related keywords