Quick Details of Six High-pressure Hose Wire Entanglement
Place of Origin: | China (Mainland) | Size: | DN25-DN200 |
Specifications of Six High-pressure Hose Wire Entanglement
Six high-pressure hose wire entanglement
High pressure steel wire braided rubber hose
your satisfaction is our pursuit...
CONSTRUCTION This hose consists of an inner tube of oil syn-thetic rubber,six spiral wire reinforcements,and an oil and weather resistant synthetic rubber cover.
APPLICATIONSHose range suitable to carry hydraulic fluids such as gly-col,mineral oils,fuels,lubricants,emulsion,hydrocar-bons etc.
The Technical Parameters of Six High-pressure Hose Wire Entanglement
Hose size | Inside Diameter mm | Reinforcement Diameter (mm) | Outside Diameter (mm) | Work Pressure (MPa) | Proof Pressure (MPa) | Burst Pressure(Pb) | |||
Mpa | Psi | MPa | Psi | Mpa | Psi | ||||
6sp-6-110 | 6±0.5 | 16.6±0.8 | 20.6±1.0 | 110 | 15939 | 220 | 31876 | 440 | 63756 |
6sp-10-77 | 10±0.5 | 21.8±0.8 | 25.8±1.0 | 77 | 11157 | 154 | 22314 | 308 | 44628 |
6sp-13-66 | 13±0.5 | 24.8±0.8 | 28.8±1.0 | 66 | 9563 | 132 | 19126 | 264 | 38252 |
6sp-16-61 | 16±0.5 | 29.0±0.8 | 33.0±1.0 | 61 | 8839 | 122 | 17678 | 244 | 35356 |
6sp-19-60 | 19±0.5 | 33.0±0.8 | 37.0±1.5 | 60 | 7390 | 102 | 14780 | 204 | 29560 |
6sp-25-50 | 25±0.8 | 39.0±0.8 | 44.0±1.5 | 50 | 5651 | 78 | 11302 | 156 | 22604 |
6sp-32-45 | 32±0.8 | 47.0±0.8 | 50.4±1.5 | 45 | 5072 | 70 | 10144 | 140 | 20288 |
6sp-38-45 | 38±1.0 | 54.2±1.0 | 57.6±1.5 | 45 | 4057 | 56 | 8114 | 112 | 16228 |
6sp-51-45 | 51±1.0 | 67.2±1.0 | 70.6±1.5 | 45 | 3188 | 44 | 6376 | 88 | 12752 |
Packaging & Delivery
Packaging Detail:Plastic films
Delivery Detail:25days
- Q: Why should the high pressure hydraulic tube peel off the outer skin?
- High pressure hose is generally relatively thick, there are steel wire layer, the purpose of peeling is to connect the tooth and steel layer close combination, the joint is more solid. But not all high-pressure hose needs peeling. Now many large companies do not need peeling. For example, pike.
- Q: Why does Br2 corrode rubber tubes?
- Bromine elements need to be sealed with water to prevent steam escaping and harm the human body. Oxidizing, there are a variety of variable valency, under normal temperature and weak water reaction, generating hydrobromic acid and bromate. Heating increases the speed of reaction. Hydrobromide is a strong acid with an acid stronger than that of hydrogen chloride. Bromine is commonly used in organic synthesis.
- Q: Pipe rubber shock absorber: flexible joints and flexible connections are not the same thing
- Flexible joint is a kind of special joint. Its performance characteristics can be generated by transverse, axial and angular displacement when it is installed. It is not limited by the pipe and the flange is not parallel. Generally, rubber parts reinforced with fabric are composed of flat movable fittings, loose metal flanges or threaded pipe flanges. They are used for vibration isolation, noise reduction and compensating displacement of pipes.
- Q: Difference between non-standard rubber joint and national standard rubber joint
- Rubber joint national Ministry of water conservancy is standard CJ/T208-2005 documents of rubber joint standard, this paper has clear rules for the product, identify the products should meet the following characteristics: standard rubber joint extrusion is produced by the rotation of the screw, the glue is advancing, and with the help of the mouth, but the needs of various semi-finished extrusion the shape of the. The extrusion process is characterized by uniform and compact quality and easy conversion of semi-finished product specifications and section shapes. The extrusion process of the national standard rubber joint in the extruder is divided into two parts: one is the extrusion system used for pushing the rubber; the two is the die system, which is used to form the rubber to make a definite section shape. Therefore, in the process of pressing, the rubber layer is usually more than ten layers, and the rubber joint has the characteristics of compact structure and high pressure resistance.Non-standard rubber joint is in the national standard between substandard products and national standard products, often illegal businesses use to reduce the rubber joint, the number of layers to reduce the cost of rubber joints. Use non-standard products instead of GB products. Non-standard products in use process, because the arc bearing layer, rubber layer is insufficient, the strength drops, in the use process is easy because the pressure withstanding insufficient causes the pipe network to burst.
- Q: Hydraulic quick change joint (external thread) how to connect and seal with hose? Do you need a transition joint?
- General hydraulic quick change joint is to withstand high pressure, so most of the situation is to use high pressure tubing, both ends of the pipe is to do the internal teeth, so it should be able to directly connect it.
- Q: The gas water heater uses metal pipes and rubber pipes
- Metal pipes are good. Rubber tubes are easy to fall off
- Q: The selection of valves and fittings has the following requirements
- The selection of hose inner screw thread joint can be rotated, because not hose and the joint body can rotate freely after buckling, configuration of internal thread after disassembly for hose.
- Q: Automotive applications of rubber hose
- Each kind of rubber has its characteristic, therefore is specially important in the hose material selection. Basically the high-end cars use materials is relatively good, some poor materials using mini car, van, car and as some in the use of nitrile rubber as fuel tube, nitrile rubber are not suitable for fuel system. Thus, the substitution of epichlorohydrin rubber fluorine rubber hose is relatively extensive.
- Q: Laboratory condensate water pipe must use rubber tube, shall not use latex tube reasons
- Hydraulic test verification pressure test: Test hose and assembly under verification pressure, continue 30s-60s, whether to produce leakage, deformation and damage. Compression deformation test: keep 1 minutes under the specified pressure (work pressure, verification pressure or other pressure below the proof pressure), measure the length and diameter of the hose, twist angle and bend. Bursting pressure test: Determination of the pressure at which the hose burst during the specified step-up rate.
- Q: How can the tightness of rubber tube and metal pipe joint be ensured?
- To see what kind of material hose, small 1MM~2MM, if the inner pressure then add hoop.
1. Manufacturer Overview
Location | Qingdao, China |
Year Established | 2002 |
Annual Output Value | Above US$ 1.5 Million |
Main Markets | Mid East, Africa, Europe, America |
Company Certifications | ISO 9001:2008; |
2. Manufacturer Certificates
a) Certification Name | |
Range | |
Reference | |
Validity Period |
3. Manufacturer Capability
a) Trade Capacity | |
Nearest Port | Qingdao |
Export Percentage | 80% |
No.of Employees in Trade Department | 260 People |
Language Spoken: | English; Chinese; Spain; Alabic |
b) Factory Information | |
Factory Size: | Above 15,000 square meters |
No. of Production Lines | 4 |
Contract Manufacturing | OEM Service Offered; Design Service Offered |
Product Price Range | Average |
Send your message to us
Six High-pressure Hose Wire Entanglement
- Loading Port:
- China Main Port
- Payment Terms:
- TT or LC
- Min Order Qty:
- 1000M m
- Supply Capability:
- 80000m per month m/month
OKorder Service Pledge
OKorder Financial Service
Similar products
Hot products
Hot Searches
Related keywords