Specifications of Geomembrane
1) Thickness : 0.15mm - 4.0mm.
2) Width : Within 8 m (1m-8m).
3) Length : 50m-100m/roll (as request).
4) Material : HDPE,( LDPE, LLDPE, PVC, EVA ).
5) Color : Black , white , red , blue , or as required.
6) Optional surface : Textued(one or two side) or smooth surface.
7) The biggest geomembrane liner manufacturer/factory in China for many years .
Geomembrane specifications
1) Thickness : 0.15mm - 4.0mm.
2) Width : Within 8 m (1m-8m).
3) Length : 50m-100m/roll (as request).
4) Material : HDPE,( LDPE, LLDPE, PVC, EVA ).
5) Color : Black , white , red , blue , or as required.
6) Optional surface : Textued(one or two side) or smooth surface.
7) The biggest geomembrane liner manufacturer/factory in China for many years .
HDPE geomenbrane Features
Good mechanical properties, high tear strength, deformation and adaptable, puncture resistance, anti-aging, anti-ultraviolet-resistant, Anti oil and salt, pH, anti-corrosion, high temperature-resistant, non-toxic, long service life. water, drainage, seepage, the good effect of moisture, width, thickness of the full range of specifications and low cost, simple construction.
HDPE Geomembrane Applications
1) Environmental protection, sanitation (such as solid waste landfills, sewage treatment plants, power plants Chi-conditioning, industrial, hospital solid waste, etc.) .
2) Water (such as rivers, lakes and reservoirs of the anti-dam, plugging, reinforcement of the canal seepage, the vertical wall of the heart, slope protection, etc.).
3) Municipal Engineering (subway, on the ground floor of the building, planted roof, the roof garden of anti-seepage, sewage pipes lining, etc.).
4) Landscape (man-made lake, river, reservoir, golf courses reservoirs of the substrate, slope protection, green lawn of the waterproof moisture, etc.).
5) Petrochemical (chemical plants, oil refineries, gas storage tanks of the anti-chemical reaction tanks, sedimentation tanks of the lining, etc.).
6) Mining (washing and pool heap leaching, the ash-field, dissolved, precipitation, the yard, the tailings seepage substrates, etc.) .
HDPE geomembrane technical index
No. | Item | Test Value | ||||||
0.75mm | 1.0 mm | 1.25 mm | 1.5 mm | 2.0 mm | 2.5 mm | 3.0mm | ||
1 | Minimum Density(g/cm³) | 0.939 | ||||||
2
| Tensile Property | |||||||
Strength at yield,N/mm | 11 | 15 | 18 | 22 | 29 | 37 | 44 | |
Strength at break ,N/mm | 20 | 27 | 33 | 40 | 53 | 67 | 80 | |
Elongation at yield,% | 12 | |||||||
Elongation at break,% | 700 | |||||||
3 | Tear Resistance N | 93 | 125 | 156 | 187 | 249 | 311 | 374 |
4 | Puncture Resistance N | 240 | 320 | 400 | 480 | 640 | 800 | 960 |
5 | Stress Crack Resistance, hrs | 300 | ||||||
6 | Carbon Black Content, % | 2.0-3.0 | ||||||
Carbon Black Dispersion | 1 or 2 | |||||||
7 | Standard OTI Min | 100 | ||||||
High Pressure OTI Min | 400 | |||||||
8 | Impact Cold Crack at -70°C | Pass | ||||||
9 | Water vapor permeability (gNaN/cm2 .s.Pa) | ≤1.0×10-13 | ||||||
10 | Dimensional Stability (%) | ±2 |
FAQ:
- Q1: Can you provide a sample for us?
A:Yes,We can send free samples,but customer need to pay the freight.
HDPE Geomembrane Price
- Q2: What is your minimum order quantity?
A:The minimum order quantity is 5000 ,but it is negotiable.
HDPE Geomembrane Price
- Q3:What is your payment terms?
A: T/T,Western Union,Paypal,L/C...
HDPE Geomembrane Price
- Q4:What is your delivery time?
A:Production time usually costs 2-20 days.
Gemembrane Show:
- Q: Is the plastic wrap toxic?
- It depends. Healthy application method of the preservative film. Warm reminder: Most of the cooked food in the supermarket is wrapped with a layer of preservative film, and many consumers think it is a protective film and directly put the food in the refrigerator when going back home. In fact, its preservative film should be torn off before storing. When consumers go back home, they should tear off the preservative film, wrap the food with freshness protection package and then put the food into the refrigerator; they can also store food in the covered ceramic containers; if the container have no cover, when cover it with preservative film, try not to put into too much food to prevent the food from contacting with the preservative film. Finally, I want to remind you that when the food is hot, do not cover it with plastic wrap, because that will increase the loss of vitamins in food. It is best to wait until the food is cooled completely before using the preservative film.
- Q: What are the key properties of a high-quality geomembrane?
- The key properties of a high-quality geomembrane include durability, flexibility, chemical resistance, and impermeability.
- Q: What is the cost of a geomembrane installation?
- The cost of a geomembrane installation can vary depending on various factors such as the size of the area, type of geomembrane material used, site conditions, and labor costs. It is best to consult with a professional installer or contractor to get an accurate estimate for your specific project.
- Q: What are the installation requirements for geomembranes in landfill caps?
- The installation requirements for geomembranes in landfill caps typically include proper site preparation, adequate slope and drainage design, surface preparation, and the use of appropriate materials and techniques for securing the geomembrane to the underlying layers. It is also essential to follow industry standards and regulations for quality control and inspection during the installation process to ensure the long-term effectiveness of the landfill cap system.
- Q: Are geomembranes permeable to water?
- No, geomembranes are not permeable to water.
- Q: What are the sticking methods of computer film?
- , first step of film sticking: aim the film marked ① at the screen and pull the ① layer of release liner label, slowly tear a part of this layer, pay attention not to touch the adsorbed layer (middle layer) of the protective?film with fingers. Second step of film sticking: aim the adsorbed layer at the screen corner, make sure that the position is aligned, smooth the film carefully while tearing off the backing layer ① release liner. Because present protective film has electrostatic automatic adsorption function, generally it does not need be ironed too much. The action should be slow when sticking the film, and it is recommended to start sticking along the long side of the screen, from point to line, from line to surface successively
- Q: Mechanism of geomembrane
- Increases the friction coefficient of contact surface. not only increases the tensile strength and puncture resistance of plastic film. Salt erosion. The main mechanism is to cut off earth leakage passage by using imperviousness of plastic film. used in the dark conditions:. // g, bearing hydraulic?pressure and adapting to dam deformation with its great tensile strength and elongation, not afraid of acid. baidu; and non-woven cloth is also a kind of high-molecule short fiber chemical material. At the same time, has long service life, through needle punching or hot sticking forming, in favor of the stability of composite geomembrane and protective layer, after being combined with plastic film, and because of rough surface non-woven fabric.baidu, alkali, they have good corrosion resistance to bacteria and chemical reaction, has high strength of extension and extensibility.
- Q: How do geomembranes contribute to erosion control in dam and reservoir construction?
- Geomembranes contribute to erosion control in dam and reservoir construction by acting as a barrier between the water and the underlying soil. They prevent water seepage, reduce soil erosion, and stabilize the slopes of the dam or reservoir. This helps to maintain the integrity of the structure and minimize the risk of erosion-related issues such as leakage or failure.
- Q: How are geomembranes used in environmental protection?
- Geomembranes are used in environmental protection as a versatile and effective barrier to prevent the contamination of soil and water. They are commonly employed in applications such as landfill liners, pond liners, and containment systems for hazardous waste. By acting as a barrier, geomembranes prevent the migration of pollutants, preventing harm to the surrounding environment and ensuring the safety of humans and wildlife.
- Q: How to deal with oil slick on fish tank?
- Oil slick processing methods: 1. Using the oil slick processor to make the oil slick into the filter, and then using the filtering?cotton in the filter to adsorb, at last decomposing bacteria by nitrobacterium. 2.Collect oil slick in the cup slowly and then dump it. 3. Use oil-absorbing sheet to absorb, put an oil-absorbing sheet at the opposite corner(oil-slick aggregated area) of water outlet to absorb oil slick. 4. Install trumpet funnel commingler to absorb oil slick, mix it with water, and it will be decomposed through absorption by filtering?cotton. 5. pump?up the planted aquarium at night after lights off 6. Remove contamination in the filter.
Send your message to us
PVC Geomembrane Pool Liners by Biggest Lining Factory in China
- Loading Port:
- Qingdao
- Payment Terms:
- TT OR LC
- Min Order Qty:
- 5000 m²
- Supply Capability:
- 2000000 m²/month
OKorder Service Pledge
OKorder Financial Service
Similar products
Hot products
Hot Searches
Related keywords