• 1.5m width PP perforated release film with high temperature for autoclave System 1
  • 1.5m width PP perforated release film with high temperature for autoclave System 2
1.5m width PP perforated release film with high temperature for autoclave

1.5m width PP perforated release film with high temperature for autoclave

Ref Price:
get latest price
Loading Port:
Shanghai
Payment Terms:
TT OR LC
Min Order Qty:
1000 roll
Supply Capability:
100000 roll/month

Add to My Favorites

Follow us:


OKorder Service Pledge

Quality Product, Order Online Tracking, Timely Delivery

OKorder Financial Service

Credit Rating, Credit Services, Credit Purchasing

Quick Details

Material:PE

Type:Release Film

Usage:vacuum forming releasing

Feature:Moisture Proof

Hardness:Soft

Processing Type:Blow Molding

Transparency:TRANSLUCENT

Place of Origin:Shanghai, China

Brand Name:TOBS

Model Number:micro perforated release film

Thickness:30μ,50μ

material:PE/PP

pore diameter:0.8mm ±0.2mm

pitch:8mm±0.1mm

Working temperature:125 /150

Tensile strength:>25MPa

Elongation:>200%

Width:1.5m ±2mm

length:ccording to the request

Product name:release film

 

 

1,Description

 Perforated Realease Film contacts with laminate directly, separating laminate and peel ply which has no release property.

2,Properties of products

Items

Description

Properties

1

material

PE/PP

2

 pore diameter

0.8mm  ±0.2mm

3

 pitch

8mm±0.1mm

4

Thickness

30μ, 50μ
 
 

5

Max. working temperature

125 /150

6

Tensile strength

>25MPa

7

Elongation

>200%

8

Width

1.5m ±2mm

9

length

 According to the request 

Q: Do you know if there is a computer screen that can be seen only from the front?
In fact, the positive is not very clear, bad for the eyes,Yes, the computer city can buy, not expensive, more than 20 yuan.
Q: How to prevent the protective film from damage and the stainless steel from marks when drawing the steel?
The surface quality of drawing dies of stainless steel is highly required. Rough surface can decrease friction and increase the property of adhesive resistance. Therefore, after the grinding processing, the more important work is to remove the processing marks left on the drawing dies. However, few people know the importance of the grinding and polishing processes when making dies. Throughout the whole process, the proportion of grinding and polishing processes should reach one third because the appearance quality of stainless steel products,to a large extent, is determined by the grinding and polishing techniques of making dies. The rougher the surface of dies is, the less it needs re-grinding. And the life of the dies also extends accordingly. If the surface of dies is not well grinded and polished, the marks on the drawn products will be clear. Although there's something to do with the fact that drawing stainless steel can easily cause seizing tumour, too. And to polish these marks takes time and the result is not good. Thus we should pay more attention to the grinding and polishing processes. Only when the surface processing precision of dies improves, can the marks decrease and the life of dies extend. In recent years, various new polishing techniques and polishing tools have arised at home. New processes and equipments such as ultrasonic polishing, electropolishing, abrasive jet and extrusion honing have been developed.
Q: PET protection film sticking is not firm, how to solve?
Rainbow pattern is now PET protection film material often encountered problems, because PET protective film material surface hardening treatment, hardening is to be treated by high temperature,
Q: There are two screens in the computer screen. One side says "A", and the other is "B". Do you need to paste A first and then paste B? Do you have two at a time? Thank you
2. the adsorption layer at the screen corner, make sure the position of alignment, while tearing, back from the film layer on the side of caution to heal, because now the protective film has automatic electrostatic adsorption function, do not need too much wait. The film moves slowly, along the long edge of the screen that a surface, from point to line, from line to surface in order to start.
Q: If the keyboard protective film is too big, do I need to cut it?
It depends on you. But you should be careful if you really want to cut it. You know there may be bulges on the edeg of the film after you cut it. The side with those bulges should be put upwards.
Q: Buy the security door, the window of the protective film, how can you quickly tear down? A long time, have some bad tear
4. With hand cream. First, the surface of the printed products tear off, and then put some hand cream on top, slowly rub with your thumb, rub for a while, you can rub the residual gum are rubbed down. Just slow down. Hand cream is a kind of grease, which is not compatible with gum. Remove glue is to use this characteristic.These third and fourth are introduced in the Central Television 1. The material is easy to find and convenient to remove.5, with banana water. Is used to remove paint an industrial agent, it is very easy to buy (sell paint there is a place to sell). The method is the same as alcohol acetone. With a hot towel in the scraping blade and eraser very clean home. Fengyoujing. It's a good thing, and it can easily solve your problem. Pay more attention to your life.
Q: What's anti-blue-ray film used for?
It has function of anti-ultraviolet-rays that can reflect visible light of harmful rays of 380nm-420nm and short wave blue ray. It's 100% anti-ultraviolet-rays of UV400. It can protect the eyes in particular.
Q: Is it necessary to peel off the protective film on the refrigerator?
You should peel it off. It's used to prevent scratches on the shell during transpotation. Firstly, it affects the appearance. Secondly, it affects heat dissipation.
Q: Is there protective film on the front side of tempered glass film?
No, there's no protective film but a layer of glass.
Q: What to do if the sandblasted protective film on marble stele is not adhesive any more?
The reasons may be: 1. If there is oil or water on the surface of the processed stele, the film can't be sticked firmly. 2. Maybe the adhesion of the protective film is not enough. I suggest you try a new film that is more adhesive. We have recieved many similar complaints from our customers. Generally, we will provide them with a variety of protective films for testing.

Send your message to us

This is not what you are looking for? Post Buying Request

Similar products

Hot products


Hot Searches