Welding Wite CO2 Gas Shielded Welding Wire Factory

Welding Wite CO2 Gas Shielded Welding Wire Factory

Ref Price:
get latest price
Loading Port:
Tianjin
Payment Terms:
TT OR LC
Min Order Qty:
100 m.t.
Supply Capability:
100000 m.t./month

Add to My Favorites

Follow us:


OKorder Service Pledge

Quality Product, Order Online Tracking, Timely Delivery

OKorder Financial Service

Credit Rating, Credit Services, Credit Purchasing

Quick Details

Place of Origin:

Hebei, China (Mainland)

Brand Name:

cnbm

Model Number:

er70s-6

Material:

CO2

Diameter:

0.8 1.0 1.2mm

Melting Point:

2700

Weight:

5kg 10kg 15kg

Application:

for welding low carbon steel,light gauge sheet,structures

Flux Content:

0.03

AWS:

ER70S-6

GB:

ER50-6

color:

golden

Packaging & Delivery

Packaging Details:black plastic spool+layer winding welding wire+tarnish paper+plastic packing+carton 15kg:72cartons on a pallet,one 20FT container can loading 20-25tons
Delivery Detail:with15-20 days

 MS flux cored welding wrie  for boiler welding :

The series of welding wries can be used to welding low carbon steel and low alloyed steel structure, such as ships, vehicles, bridges, boilers and buildings etc.

package:5kg,15kg,20kg

have excellent mechanical performance such as fast melting rate, high depositing efficiency, stable arc, little spatter, beautiful seam. Suitable for all-position welding work.

Specifications of welding wire:

1) Sizes: 0.8mm,0.9mm,1.0mm,1.2mm,1.6mm

2) Applications: Widely used as welding carbon steel wires in shipbuilding,

Bridge building, machinery manufacturing and general welding purposes


 

Mechanical properties of deposited metal

 

C

Si

Mn

P

S

Cr

≤0.10

0.80~1.15

1.40~1.85

≤0.02

≤0.02

≤0.10

Ni

Cu

Al

Co

Ti

V

≤0.10

≤0.30

≤0.01

≤0.01

≤0.01

≤0.02

 

 

 

Mechanical properties of deposited metal

Yield stregth(Mpa)

Tensile strength(Mpa)

Elogtions(%)

Impact value (J)

≥400

≥480

≥22

≥27

picture

Welding Wite CO2 Gas Shielded Welding Wire Factory

Welding Wite CO2 Gas Shielded Welding Wire Factory

Welding Wite CO2 Gas Shielded Welding Wire Factory

Welding Wite CO2 Gas Shielded Welding Wire Factory

Welding Wite CO2 Gas Shielded Welding Wire Factory

Welding Wite CO2 Gas Shielded Welding Wire Factory



Q: I know there are trace elements in the welding wire, but how can I identify them?
It doesn't make much difference. The welding wire is the steel wire, and the steel wire is not necessarily the welding wire
Q: Q235 plate thickness 4mm-5mm what is the diameter of the wire to be selected by submerged arc welding what is the flux?
In fact, 4-5MM has a special submerged arc welding 1.6 wire, that is automatic two welding machine, remove gas and welding flux. Or use 2.5 of the wire,
Q: What gas welding flux cored wire?
Flux cored wire is formed by cold drawn after the steel strip contains deoxidizer, arc stabilizing agent and other component powder. It is also called tubular welding wire. Usually under the protection of carbon dioxide gas or argon + carbon dioxide gas, and there is no need for gas protection, also known as self-protection.
Q: What welding wire should be used when welding between 0cr18Ni9 and 0cr18Ni9?
Base metal 0Cr18Ni9, welding rod A137, argon arc welding wire H0Cr20Ni10.1, welding wire is used as filler metal or as a conductive wire welding material.2, in gas welding and gas tungsten arc welding, welding wire used as filler metal; in submerged arc welding, electroslag welding and MIG arc welding, welding wire as filler metal, and conductive electrode. The surface of the wire is not coated with anti oxidizing flux.
Q: Welding rod welding wire preservation many time failure cannot use, has this aspect stipulation? Is the electrode qualified for more than one year after reinspection?
Should be okay?
Q: ZG40Mn how to weld 70 wire that I use, preheat before welding, keep warm after welding, still appear crack
How warm are you? ZG40Mn welding performance is very poor, whether to consider welding wire MG600 MG660 (I have not tried 70 wire welding ZG40mn)
Q: What is the distance between the welding nozzle and the template for argon arc welding?
The wire feed is delivered to the edge of the bathOne drop at a time,When you return it, you can not withdraw from the argon protection range.
Q: 3003 what welding wire for aluminum plate?
Aluminum silicon 4043 or aluminum magnesium 5356 wire can try
Q: Can ER308 welding wire be replaced by ER321?
ER308 welding wire can be replaced by ER321.ER308's national brand is H08Cr21Ni10Si;ER321's national brand is H08Cr19Ni10Ti;Compared with ER308, Cr-Ni element has little difference, but only adding stabilizing element Ti to ER321 can improve the intergranular corrosion resistance of ER321 welding seam.Welding wire is used as filler metal or metal wire welding material at the same time as conductive. In gas welding and gas tungsten arc welding, welding wire used as filler metal; in submerged arc welding, electroslag welding and MIG arc welding, welding wire as filler metal, and conductive electrode. The surface of the wire is not coated with anti oxidizing flux.
Q: What is the problem of welding when the material is different from the wire?
This is a ahFirst, the parent material, copper, aluminum, carbon steel, stainless steel, cast iron, titanium,,,,,Besides welding material,,,,,,,,And then discuss the welding methodThen arrange them together.Can be welded, divided into categories.Not soldered, in one class.