• Silicon Bronze Tig Welding Wire Rod for Building System 1
  • Silicon Bronze Tig Welding Wire Rod for Building System 2
  • Silicon Bronze Tig Welding Wire Rod for Building System 3
Silicon Bronze Tig Welding Wire Rod for Building

Silicon Bronze Tig Welding Wire Rod for Building

Ref Price:
get latest price
Loading Port:
Qingdao
Payment Terms:
TT or LC
Min Order Qty:
10 m.t.
Supply Capability:
1000 m.t./month

Add to My Favorites

Follow us:


OKorder Service Pledge

Quality Product, Order Online Tracking, Timely Delivery

OKorder Financial Service

Credit Rating, Credit Services, Credit Purchasing

Characteristics

1)Pure aluminum -99% min 
2)Excellent corrosion resistance. 
3)High thermal conductivity and electrical conductivity.

Quick Information:

Class: ER1100

AWS: A5.10

Conforms to Certification: AWS A5.10                 ASME SFA A5.10

Weld Process: Tig (GTAW)

 

Specifiaction:

AWS Chemical Composition Requirements
Cu = 0.05 – 0.20Al = 99.0 min
Mn = 0.05 maxSi + Fe = 0.95 max
Zn = 0.10 maxBe = 0.0003 max
Other = 0.05 each – 0.15 total

Available Sizes:
Upon Request, call for more information

 

Application:
Type ER1100 can be used to weld base materials types 1060, 1070, 1080, and 3003.

  • Welding Filler Wire

  • Heat Exchangers

  • Food Handling Equipment

  • Rivets

FAQ:

The proper choice of aluminum filler metal mainly depends on the base metal properties to be achieved and welding technique. Post weld cracking, corrosion resistance and behavior under elevated temperature also need to be taken into consideration. Cracking usually can be minimized by choosing a filler metal alloy of higher alloy content then the base metal.

Deposited Chemical Composition % (Typical)
Deposited chemistry is influenced by many factors so no typical analysis can be reported.

Deposited All Weld Metal Properties %


Pictures:

Silicon Bronze Tig Welding Wire Rod for Building

Silicon Bronze Tig Welding Wire Rod for Building

Silicon Bronze Tig Welding Wire Rod for Building


Q: How does the camera shoot under the tungsten lamp?
F If you take stills, usually 5.6 or less, if the film moving pull, you can go to 18,22, the shutter is appropriate to make their own satisfaction with the picture prevail
Q: The effectiveness of magnetron and the comparison of pure tungsten wire heating
For the magnetron is the identification of aging, the traditional method is to measure the filament resistance, under normal circumstances should be less than 1Ω, and the smaller the better.
Q: Clean the toilet with tungsten wire brush the toilet when the toilet into a black how to do
Because the cleanser is acidic substances and active metal chemical reaction, resulting in acid salt easily adsorbed on the ceramic surface. Later use clean lanterns to avoid the use of metal tools.
Q: What is tungsten wire?
It is also necessary to incorporate a small amount of potassium, silicon and aluminum oxides in the process of metallurgy, which is called DopedTungstenWire, also known as 218 tungsten wire or non-sagTungsten wire (Non-sagTungstenWire).
Q: Tungsten wire bulb with a long time why black
The tungsten wire is gasified at high temperature and is attached to the inner wall
Q: Tungsten wire can not use DC?
Tungsten filament whether it is DC or AC, as long as it can reach its operating voltage, can be used
Q: How will the tungsten melt?
It is because it is high melting point made bulb filament
Q: Why is the spectrum of tungsten filament incandescent?
With a continuous spectrum of light through the low-pressure gas, the corresponding position appears discrete black line.
Q: Led lamp in the tungsten wire and the relationship between the wire
LED lights in imitation tungsten lamp, there are two kinds of materials: ceramics and sapphire
Q: Nickel-chromium alloy wire and tungsten wire which is good?
See what you are doing! Filament is the high melting point with tungsten wire

Send your message to us

This is not what you are looking for? Post Buying Request

Similar products


Hot Searches

Related keywords