General information of low carbon wood
Raw material |
Sawdust, corn-straw and tailing, can be recycled after using. |
Technology |
Utilizing molecular structure of crystalline-state solidification, shaping under normal temperature and pressure with low carbon emission. |
Installation |
Stitching, wet-sticking and dry-fasten connecting |
Character |
Favorable corrosion resistance, non-ignitable, water-proof, UV-resistant, high resistance to fire, water and insects. |
Lead time |
30 days after receiving buyer's original L/C or Prepayment |
Package |
Seaworthy Export Standard Wooden Pallet |
Four breakthroughs |
Comprehensive utilization of natural resources: Be recyclable, using sawdust, corn-straw and tailing as materials. The product can be recycled after using. |
Low carbon and energy saving in the course of production: Adopting the independent individual property’s technology, utilizing molecular structure of crystalline-state solidification, shaping under normal temperature and pressure with low carbon emission. | |
Environmental and healthy in the course of construction and using: Synthesized by natural inorganic raw materials, nontoxic, odorless and non-radiative simple installation, which could save energy cost and reduce and waste emission, raise efficiency and reduce erection time. | |
From nature, beyond nature: Full realization of the natural texture, high resistance to fire, water and insects. Do not rot or fade after long time usage. Super self-cleaning needs low maintenance cost. Vivid color and appearance provides a wide space to designers. | |
Six advantages |
Lower more than 50% cost, enhance building's performance to price ratio. |
Cutting at will, Fixing easy, Shorting project time. | |
Good performance in resistance to elements, corrosion-resistant ,resistance to termite, fire resistance and water-resistant, far from distortion and discolorations in 30 years. | |
Well self-cleaning, low cost in later maintenance: Don't need professional maintenance in 30s(Cleaning with water only), saving much cost. | |
Customize the color, showing individuation: Beyond 400 kinds of colors, designers could exhibit their imagination. | |
Compound with natural inorganic materials: Without formaldehyde and toluol, sustained releasing negative oxygen ion, forming nature oxygen bar. | |
Special specifications are available on customers' requirements. |
Specification of low carbon wood
Standard: 3000mm(L)×1200mm(W)×15mm(T)
Standard length: 3000mm
Standard width: 120mm,150mm,200mm,300mm(including 3mm kerf width)
Standard thickness: 15mm
Technical information of low carbon wood
Density |
1.26g/m3 |
Folding strength |
10Mpa |
Dry-shrinkage rate |
0.05% |
Elastic modulus |
7211Mpa |
Wet expansion rate |
0.17% |
Shear strength |
3.5Mpa |
Screw holding capability |
121N/mm |
Coefficient of heat conductivity |
0.69(W(m·k)) |
Frost resistance |
Thaw-freeze cycle after 30 times, no slip crack and peeling off | ||
Unpermeability |
No drop appearing on the bottom after 24 hours. | ||
Impact strength |
3.3KJ/m2 |
Products exhibition of low carbon wood
Low carbon wood sheets with thin grain
Low carbon wood sheets with thick grain
Project picture of low carbon wood
- Q: Simple construction method of veneer
- With fine sandpaper along the veneer pattern grind joints, so that seams traces down
- Q: Slicing of thin slices of wood
- after cooking treatment; the cooking process should be reduced to more than 40 ℃, it should slow down the heating rate
- Q: The following table lists the cooking criteria for several types of wood,
- After drying moisture content is generally required in 8% to 12% is appropriate, thin wood drying equipment with continuous operation of the drum dryer and belt dryer
- Q: What can the veneer be classified?
- according to the manufacturing method of classification Can be divided into sliced thin wood; peeling veneer; sawing thin wood; semi-circular peeling veneer. Often the use of slicing method
- Q: The principle of veneer dyeing
- Dyed veneer production process by screening high-quality imported veneer, the use of high-tech processing technology to take off the veneer in the impurities and mineral lines
- Q: Veneer should pay attention to the different production processes
- First of all, in our country will be used for wood veneer furniture, veneer materials, furniture manufacturing enterprises More and more,
- Q: The Production process of cooking
- The following table lists the cooking criteria for several types of wood, for reference only.
- Q: Veneer has a very affordable, versatile features
- With the current shortage of natural timber resources, as well as the price of high-grade tree species is climbing
- Q: What is the size of the veneer?
- Veneer short material, long material and large sheet material. 1 meter to 2 meters is generally referred to as short material, 2 meters to 2.45 meters is generally known as long material
- Q: The Sliced ??veneer manufacturing process
- Wood → truncated → cut → softened (steamed or boiled) → slicing → drying (or not drying) → cutting → inspection packaging → storage
Send your message to us
Architectural Wood Veneers - High Quality Low Carbon Wood 005
- Loading Port:
- China Main Port
- Payment Terms:
- TT or L/C
- Min Order Qty:
- 1000 sq.m, m²
- Supply Capability:
- 400000 sq.m. Per Month m²/month
OKorder Service Pledge
OKorder Financial Service
Similar products
Hot products
Hot Searches