• Fiberglass Mesh Cloth - 45gsm, 5mm*5mm Resistant Fiberglass Marble Mesh for Buildings System 1
  • Fiberglass Mesh Cloth - 45gsm, 5mm*5mm Resistant Fiberglass Marble Mesh for Buildings System 2
  • Fiberglass Mesh Cloth - 45gsm, 5mm*5mm Resistant Fiberglass Marble Mesh for Buildings System 3
Fiberglass Mesh Cloth - 45gsm, 5mm*5mm Resistant Fiberglass Marble Mesh for Buildings

Fiberglass Mesh Cloth - 45gsm, 5mm*5mm Resistant Fiberglass Marble Mesh for Buildings

Ref Price:
get latest price
Loading Port:
China main port
Payment Terms:
TT OR LC
Min Order Qty:
1000 m²
Supply Capability:
300000 m²/month

Add to My Favorites

Follow us:


OKorder Service Pledge

Quality Product, Order Online Tracking, Timely Delivery

OKorder Financial Service

Credit Rating, Credit Services, Credit Purchasing

45gsm,5mm*5mm Alkali Resistant Fiberglass Marble Mesh for Buildings

 

Definition of Fiberglass Marble Mesh

Fiberglass Marble Mesh is mainly alkali-resistant fiberglass fabric. Fiberglass Marble Mesh  mainly use the C /E-glass fiber yarn (main ingredient is a silicate, good chemical stability) through a special weaving technique, then by the anti-alkali and reinforcing agent etc high temperature heat finishing treatments. Fiberglass Mesh is an ideal engineering material in construction and decoration industry.

Image of Fiberglass Marble Mesh

45gsm,5mm*5mm Resistant Fiberglass Marble Mesh for Buildings45gsm,5mm*5mm Resistant Fiberglass Marble Mesh for Buildings

Fiberglass Marble Mesh  Production Process 

45gsm,5mm*5mm Resistant Fiberglass Marble Mesh for Buildings

Fiberglass Marble Mesh Application :

45gsm,5mm*5mm Resistant Fiberglass Marble Mesh for Buildings45gsm,5mm*5mm Resistant Fiberglass Marble Mesh for Buildings

Package: Fiberglass Marble Mesh are packed in shrink-wrapped, then put into cartons or pallets.

Packing volumes: about 20000m/20FCP, 40000m2/40HQ.

Delivery: About 15 days after confirming the order.

 

45gsm,5mm*5mm Resistant Fiberglass Marble Mesh for Buildings


45gsm,5mm*5mm Resistant Fiberglass Marble Mesh for Buildings

FAQ: 


Q: What is the Advantage of Fiberglass Mesh ?

 

Good chemical stability: Alkali-resistant, acid-resistant, waterproof, cement  erosion-resistant, and other chemicals' corrosion resistant; and strong resin bonding, soluble in styrene.

 

Outstanding craftsmanship include coating enough alkali-resist glue, our coating glue is produced by Germany BASF which can keep 60-80% strength after test in Naoh 28days later, so that guarantee high strength, high tensility, light weight.

 

Our fiberglass yarn is supplied by Jushi Group which is the largest producer of fiberglass yarn in the world like Saint Gobain, it's 20% extra strong strength and beauty surface than normal fiberglass yarn.

Strength retention rate> 90%, elongation<1%, the durability of more than 50 years.

 

Good dimensional stability & positioning property, stiffness, smoothness an difficult to shrink & deformation.

Good impact resistance and not easy to be teared.

 

 

Q: Why choose our CNBM Fiberglass Mesh?

 

We are the manufacturer of Fiberglass Mesh, price will be reasonable and much competitive

We have produced Fiberglass Mesh strictly in according to customers' detailed requirements

CNBM Fiberglass Mesh theme is: Good Quality, High Credibility & Best Service.

 

 


Q: How do you paste the mesh cloth on the back of the stone?
At the bottom of the stone board, besmear the resin glue, and then adhere to the fiber mesh cloth, forming tensile waterproof layer, but must not forget to brush in the side.
Q: Where is fiberglass mesh better?
Quality and import gap is not large, but prices are significantly lower. If you do not take the price into consideration, it must be the best of the imports.
Q: Do external insulation with alkali resistant fiberglass mesh cloth, why should the first layer be double or thickened?
The two layer and the above position can not be reached by human activities, so it is OK to adopt single layer mesh cloth.
Q: Glass fiber mesh cloth, crack mortar, tiling there is no problem?
This is absolutely no problem. Is the insurance, you, than it is to use some wall tiling grid cloth, ordinary mortar mortar is much better, but the cracking phenomenon is not so much that they...
Q: What harm does fiberglass mesh have to people?
Glass fiber can irritate the skin, cause skin irritation, itching, and may cause deeper damage.
Q: Self-adhesive fiberglass mesh
Self adhesive mesh and EPS mesh than the general viscous grid has the characteristics and general mesh fabric. But than the general mesh more viscous soft, moderate viscosity, uniform coating, adhesive does not appear in some places, some places less adhesive at the time of construction, to avoid the "bulge" phenomenon.
Q: What's the price of fiberglass mesh?
The elastic coefficient is high, the elongation within the elastic limit is related to the tensile strength of the alkali resistant fiberglass mesh cloth
Q: What is the difference between alkali resistant fiberglass mesh cloth and high alkali glass fiber mesh cloth?
Alkali resistance refers to the performance of special glass fiber, while high alkali refers to the composition of glass fiber.Are two completely different concepts.
Q: Slotted walls, seams, seams, tape, or anti mesh cloth?
Don't spend so much money to buy what tape and mesh cloth, is decorated well, to buy the cheapest dacron, remember to not want that kind of chemical fiber, cotton, cotton for a long time to decay.
Q: What is the use of alkali resistant fiberglass mesh cloth on the exterior wall?
The use of composite plaster mortar of alkali resistant glass fiber cloth, on the one hand, can effectively increase the tensile strength of the protective layer, on the other hand, can effectively disperse stress, can be originally may have wider cracks spread into many smaller cracks, thus forming the crack in. The surface coating material and the amount of coating have important significance to the alkali resistance of glass fiber mesh cloth, and the glass fiber variety has a decisive significance for long-term alkali resistance. In the process of using glass fiber mesh: mesh between lap width not less than 50mm, the negative corner mesh to pressure stubble lap, its width is larger than 50mm, yang angle is greater than or equal to 200mm. In the construction, mesh paving should be smooth, no wrinkles, mortar plumpness reached 100%, at the same time to find and maintain smooth, straight corner square and the verticality of yin and yang.