• Type Calcined Petroleum Coke System 1
  • Type Calcined Petroleum Coke System 2
  • Type Calcined Petroleum Coke System 3
  • Type Calcined Petroleum Coke System 4
Type Calcined Petroleum Coke

Type Calcined Petroleum Coke

Ref Price:
get latest price
Loading Port:
Tianjin
Payment Terms:
TT OR LC
Min Order Qty:
10 m.t
Supply Capability:
6000 m.t/month

Add to My Favorites

Follow us:


OKorder Service Pledge

Quality Product, Order Online Tracking, Timely Delivery

OKorder Financial Service

Credit Rating, Credit Services, Credit Purchasing

Quick Details

  • Place of Origin: Liaoning, China (Mainland)

  • Brand Name: CMAX

  • Application: Steel Making

  • Shape: Carbon Powder

  • Dimensions: 0-1MM 90%, 1-3MM 90%, 1-5MM 90%, 2-8MM 90%

  • Product Type: Carbon Additive

  • C Content (%): 98.5%min, 99%min

  • S Content (%): 0.5%max, 0.7%max

  • Ash Content (%): 0.5%max, 0.8%max

  • Volatile: 0.5%max, 0.8%max

  • Moisture: 0.5% MAX

  • Item Name: Petroleum Coke Type Calcined Petroleum Coke


Packaging & Delivery

Packaging Details:IN ONE MT JUMBO BAG; 
25KS SMALL WOVEN BAGS AND 4O SUCH BAGS IN A MT JUMBO BAG;
Delivery Detail:WITHIN 30 DAYS AFTER RECEIVING LC DRAFT OR DOWNPAYMENT

 

Petroleum Coke Type Calcined Petroleum Coke

General Specification of CPC/Calcined Petroleum Coke:

 

PARAMETER   UNIT GUARANTEE VALUE

F.C.%

98.5MIN 

98.5% MIN

ASH %

0.5 MAX

0.8MAX

V.M.%

0.7 MAX

0.7 MAX

SULFUR %

0.5 MAX

0.7 MAX

MOISTURE %

0.5MAX

0.5MAX

SIZE

0-5MM OR AS REQUEST

 


 

Picture of   Petroleum Coke Type Calcined Petroleum Coke


 

 

Petroleum Coke Type Calcined Petroleum Coke

 

USAGE:

Calcined Petroleum Coke is a critical ingredient in the production of Metallurgy and chemical industrial ,it can increase the used quantity of Scrap steel and reduce the quantity of Scrap iron, or use no Scrap iron at all, the calcined petroleum coke has follow properties: high absorptive character, no residue will be left and save production cost.

 

1. Usage: calcined petroleum coke is used to improve the Carbon content in steel-melting and Ductile iron foundry
2. Characteristic:high carbon, low sulfur, with stable effect for improving the carbon content, high absorptive of carbon.
3. Application:calcined petroleum coke   is used in electric furnace steel smelting and cast-iron for improving the carbon content

Petroleum Coke Type Calcined Petroleum Coke

 

We can supply below furnace charges, please feel free to contact us if you areinterested in any of any of them:
Coke (Metallurgical, foundry, gas)

 

Calcined Anthracite with fixed carbon from 90% to 95%

 

Calcined Petroleum Coke

 

Graphite petroleum coke

 

Amorphous Graphite


 

Address:No.2 Zi Zhu Yuan South Road,Haidian,Beijing, P.R.C


Q: What are the companies that produce coke
Very much, what kind of coke do you want, our company would like to buy coke particles
Q: What is the reasonable standard of volatile content of coke
11% of the sulfur from the blast furnace charge into the furnace comes from the ore, and the other comes from the limestone; the other is from the coke, so the coke is the main source of sulfur in the charge of the 82.5% of the charge. Sulfur content in coke directly affects the production of blast furnace. When the sulfur content in coke is greater than 1.6%, sulfur increased 0.1%, the amount of coke increased 1.8%, limestone amount increased 3.7%, 0.3% increase in amount of ore blast furnace output to reduce the sulfur content under 1.5 - 2.0%. metallurgical coke is not greater than 1%, the use of large and medium-sized metallurgical coke content in blast furnace is less than 0.4 - 0.7%.
Q: The total amount of heat released by the fully burnt 200g coke is 60% by mass of 10kg water absorption [q coke =3.0 * 107J/kg, C water =4.2 * 103J/ (kg = C)], q:(1) how much heat is absorbed by water?(2) if the initial temperature of water is 10 degrees C, then, after absorbing heat, the temperature will rise to how much?
(1) the amount of heat released from complete combustion of coke:Q put =mq=0.2kg * 3 * 107J/kg=6 * 106J.Heat absorbed by water:Q =Q * 106J suction ETA =6 * 60%=3.6 * 106J;(2) Q =cm t suction dreams,Dry water temperatures:Delta t=Q ceilingC water m water=3.6 x 106J4.2 x 103J/ (kg * c) * 10kgC = 85.7,
Q: China's coke iron smelting began in what time?
Han also invented the "fried steel law", that is, the use of pig iron "fried" mature iron or steel of the new process, the product is called steel. At the same time, the rise of "100 steelmaking" technology. The Eastern Han Dynasty (AD 25 ~ 220), when the emperor of the Ming Dynasty, invented the hydraulic blast furnace, that is, "water discharge". The invention of ancient water row in China, about 1100 years earlier than europe. After the Han Dynasty, the method of steel. "Qi Shu Qi, even referred to as" places "big steel", later known as the filling steel, also known as steel group. This is another important achievement of the ancient steelmaking technology in china. According to the "Encyclopedia of" records: Chinese is the earliest use of coal iron country, the Han Dynasty have been tried, song and Yuan dynasties have been popularized. To the Ming Dynasty (AD 1368 ~ 1644) has been able to use coke smelting pig iron.
Q: Why does Coke provide heat when it is fired, it reacts only at high temperatures and why it is needed to provide heat?Which is the exothermic reaction, carbon dioxide or carbon monoxide?
Generate CO2;Of course, high temperature will produce CO, but not many;Please ask questions
Q: Who knows the proportion of pig iron and coke used in Cupola
There is doubt: the export rate is lower than the standard exception.4, blank blank processing: according to customer requirements of different direct sales, some need to continue processing after the sale, the ordinary rough machined after a blank rate of about more than 70%, about 30% (excluding scrap scrap), dryer enterprises after after machining yield is about 25% ~ 30% (including waste scrap and iron, basically use recycled material, material waste accounted for ratio of 30% ~ 40%). To 1.5M x 2M cylinder, for example, rough weight of about 5.8 tons ~ ~ 6 tons (standard cylinder, including the cylinder head) cylinder head rough weight of about 1.7 tons ~ ~ 1.8 tons, cylinder weight of about about 4.2 tons. After processing, the cylinder head weighs about 0.5 tons to 0.6 tons, accounting for the proportion of about 65% to 70% head (excluding scrap, scrap accounted for about 10%, blank cylinder head and iron) accounted for about 30% ~ 35% blank cylinder head, accounted for the proportion is about 40% recycled waste, scrap iron accounted for under foot material proportion 60%, enterprises can not return direct sales (currently, only production enterprises can use recycled scrap iron). Total iron blank ratio is about 15% ~ 18%.
Q: What is the difference between coke and carbon residue? Coke is a high-temperature refining, carbon residue can be used for civilian fuel it?
Gasification coke, which is used in the production of coal gas, is mainly used in the fixed bed gas producer with solid slag, as the raw material for gasification, producing CO and H2 as the combustible component:C+O2 - CO2+408177KJCO2+C - 2CO-162142KJC+H2O - CO+H2-118628KJC+2H2O - CO2+2H2-75115KJ
Q: What are the requirements for coke and other accounts?
4, I personally set the password and password.5, the customer I own the bank transfer agreement, my ID card, bank debit card to the corresponding bank outlets for bank transfer procedures.6, the day of the day to accept the phone call Futures Company visit, after the successful return of T+1 days of commodity futures trading.7, the customer into the gold (silver period transfer; non bank transfer).8, customer online transactions (start trading).
Q: What are the criteria for coke classification and how to distinguish between primary and two grade coke?
The use of coke:Shanxi sales of various specifications of foundry coke, metallurgical coke, high sulfur coke or motor transport cars can be. The specific indicators are as follows:More than 83 of the fixed carbon; sulfur below the volatile content of less than 1.5; ash around 15 e:Mechanism coke: used in metallurgy; steel plantFiddle coke size 8cm-150cm: of molten iron for casting {;} of motor shell, radiator, mechanical counterweightCoal tar: molten iron; used in the casting of motor shell, radiator, mechanical counterweightLarge modified coke: {for ordinary casting; mechanical parts such as rough parts for 2-3.5 tons of furnace type}The shape of coke size 25cm:{is used for ordinary casting and slightly rigid casting products, such as water pump pipe fittings, such as fire fastenerMore than 85 of the fixed carbon; volatile 1.5.; ash content of less than 13.5 sulfur; less than 0.5:A fiddle coke size above 8cm for ordinary casting: {}Setting coke size 25cm; {for precision casting and ductile castingImproved coke: (Jiao Meilian) {for precision casting and ductile castingCoal tar: molten iron; used in the casting of motor shell, radiator, mechanical counterweight
Q: How to determine the maturity of coke or not?
The sulfur content of coke: refers to the percentage of sulfur content in coke. Sulfur is one of the harmful impurities in pig iron smelting. The sulfur content in the pig iron is more than 0.07%. 82.5% of the sulfur from blast furnace charge into the furnace comes from coke, so coke is the main source of sulfur. Sulfur content in coke directly affects the production of blast furnace. When the sulfur content in coke is greater than 1.6%, sulfur increased 0.1%, the amount of coke increased 1.8%, limestone amount increased by 3.7%, with the increasing of the amount of ore 0.3%, blast furnace production decreased 1.5 - 2%.

Send your message to us

This is not what you are looking for? Post Buying Request

Similar products

Hot products


Hot Searches

Related keywords