• Steel Welding Electrode with Blended AWS E6013 and Competitive Price System 1
  • Steel Welding Electrode with Blended AWS E6013 and Competitive Price System 2
Steel Welding Electrode with Blended AWS E6013 and Competitive Price

Steel Welding Electrode with Blended AWS E6013 and Competitive Price

Ref Price:
get latest price
Loading Port:
Tianjin
Payment Terms:
TT OR LC
Min Order Qty:
25000 kg
Supply Capability:
25000000 kg/month

Add to My Favorites

Follow us:


OKorder Service Pledge

Quality Product, Order Online Tracking, Timely Delivery

OKorder Financial Service

Credit Rating, Credit Services, Credit Purchasing

1.Steel Welding Electrode with Blended AWS E6013 and Competitive Price Description:

First Class WeldingElectrode Customization is welcome . We could produce various Welding Electrode.

according to buyers’drawing or samples/Non-standard Welding Electrode .The price, picture

and product attributes are for reference only. Specific matter can be confirmed

by a further communication. Welcome your consultation.

 

2.Main Features of Steel Welding Electrode with Blended AWS E6013 and Competitive Price

Fewer spatters 
Easy to restrike 
Less smog 
Good off slag,high deposition efficiency

3. Steel Welding Electrode with Blended AWS E6013 and Competitive Price Images

 Steel Welding Electrode with Blended AWS E6013 and Competitive Price

4. Steel Welding Electrode with Blended AWS E6013 and Competitive PriceSpecification 

Chemical composition

C

Mn

Si

S

P

Guarantee value

≤0.12

0.3~0.6

≤0.35

≤0.035

≤0.040

                                                      

Test Item  

Rm(MPa)

ReL(Mpa)

A(%)

KV2(J)

KV2(J)

Guarantee value

≥420

≥330

≥17

-(normal temperature)

-(0°C)

General result

460~540

≥340

18~26

50~80

≥47

 

5.FAQ

We have organized several common questions for our clientsmay help you sincerely 

1.   What’s your products 

One of the most biggest manufacturer & supplier of  Welding Electrode  is a large-scale professional  Welding Electrode  factory in China. Annually more than 10000 tons  Welding Electrode   are exported to markets all over the world. Different kinds of  Welding Electrode  are available according to customer’s requirements. 

 

2.What is advantage of our products?

All items are of Top Quality with best price. Direct wholesale price from Factory and 100%quality guaranteed .Large Selection with all sizes .

 

3.  How long can we receive the product after purchase?

In the purchase of First Class  Welding Electrode within three working days, We will arrange the factory delivery as soon as possible. The pacific time of receiving is related to the state and position of customers. Commonly 15 to 20 working days can be served.

Q: Urgently!!! The plating of nickel plating meets the soldering flux when soldering. The reaction result in the surface of the electroplated parts is pale yellow and black. How can I deal with this problem effectively and make the electroplated parts come back to its original appearance? Online results
It's definitely not going to be the way it is. It's the next thing to do, not the first time
Q: Tin on both sides of the plate, soldering flux is always can not go up, tin can not. Expert advice, how to enhance the flow of flux and tin permeability
Add more thinners
Q: How long is the soldering flux valid?
The soldering flux is stored in a cool place as long as it is sealed. The shelf life is one yearIt usually placed in tin flux in high temperature and high humidity weather encountered, often put a day for second days due to flux to absorb moisture in the air and affect the welding quality.
Q: TitleWhat is the difference between rosin flux solder paste?What is the difference between rosin, soldering flux and solder paste? What are their respective functions? Thank you
The flux is known, rosin, solder paste to use flux, the most critical is to increase the welding and welding solder objects (poor infiltration effect infiltration, solder is not well attached to the welded object, appeared a round ball, it is easy to weld), other auxiliary heat removal, such as oxidation conduction, reduce surface tension, so that the metal solder joint appearance etc.. Flux is divided into three categories: one is inorganic flux, two is organic flux, and three is rosin. Inorganic flux is generally a certain acid or salt, such as phosphate H3PO4, organic flux is mainly some organic acid or organic halogen; relatively speaking, the most active inorganic flux, remove the oxide film had the best effect, but also has strong corrosion resistance, it is easy to hurt the metal and solder joints, generally can not be used in the welding of electronic products. Solder paste is emulsified with oil after the inorganic flux, welding can be cleaned by solvent, but some parts of the circuit board is difficult to clean, so generally do not recommend the use of solder paste. Organic flux is second only to inorganic flux, and also has certain corrosiveness, and the residue is not easy to be cleaned, and the volatile matter is harmful to human body. Is the main component of rosin rosin acid and Levopimaric acid, generally neutral, liquid has a certain activity, showed weak acidity, can react with the metal oxide surface, formation of abietic acid copper compounds, and suspended in the surface of the solder, and the use of no corrosion, insulation resistance. Rosin is, in general, the best soldering flux.
Q: What is soldering flux? Is alcohol the main component of soldering flux?
Welding aid is a reducing agent which reduces metal oxides to metals and is easy to weld.
Q: Because of my article is aluminum solid core, it is not with the flux? Is there any need to add it?I am the aluminum tube in the fridge and welded to the aluminum tube
The aluminum tube and the aluminum pipe welding can be welded with ALCU-Q303, and can search the "copper aluminum welding video" in the Baidu net ALCU-Q303 how to weld the copper aluminum pipe joint
Q: I have 52 degrees of liquor (now home to drink the rest of the O (a _ a), O~) and refined rosin, how much is the allocation ratio. Look, someone uses 1:1 on the Internet. It doesn't seem to work. You must do it or understand it. No irrigation. Good answer, 10 points. By the way, am I pure alcohol?.
52 to ensure that you can put the stove up, go to the electronic city to buy industrial alcohol, methanol or isopropanol. I'm a soldering agent. I hope to help you.
Q: A LDE lamp circuit board, high temperature will cause the light shade (transparent white mist) (do not know is not clean flux or ethanol), the current solution is to get the baking oven 100 C 40min, have what good method?
The soldering flux on the PCB circuit board can be removed with an ultrasonic cleaner.
Q: The flux is sprayed on the PCB board. There is a lot of yellow on the solder joint. Which is the reason for the flux?
LZ, I suggest you let the supplier re debug, see it, make some improvements in the preparation
Q: The soldering flux is good or good hydrochloric acid with sulfuric acidWhat is the sulfuric acid soldering flux or hydrochloric acid, which is easy to use?
Industrial process for sodium hydroxide (1) filtration of sea water(2) adding excessive sodium hydroxide to remove calcium and magnesium ions and filterCa (2+) +2OH (-) =Ca (OH) 2 (slightly soluble)Mg (2+) +2OH (-) =Mg (OH): 2(3) adding barium chloride to remove sulfate ion and filter;Ba (2+) +SO4 (2-): =BaSO4(4) adding excess sodium carbonate, removing calcium ion, excessive barium ion, and filteringCa (2+) +CO3 (2-): =CaCO3Ba (2+) +CO3 (2-): =BaCO3(5) adding hydrochloric acid to remove excess carbonate ions2H (+) +CO3 (2-) =CO2 = +H2O(6) heating away carbon dioxide(7) feed into an ion exchange tower to further remove calcium and magnesium ions(8) electrolysis2NaCl+2H2O= (power) H2 = +Cl2 = +2NaOH