1. Metallurgical Coke of COKE BREEZE 0-5mm Description:
Coke is made by high temperature metallurgical coke for blast furnace smelting, casting and gasification. Occurring in the process of coking after recovery and purification of coke oven gas is a high calorific value of fuel, is an important industrial raw material in organic synthesis.
Coke is mainly used for blast furnace ironmaking and used for copper, lead, zinc, titanium, antimony, mercury and other non-ferrous metal smelting of blast furnace, reducing agent, compound and the function of stock column frame.
Blast furnace with Coke instead of charcoal, which laid a foundation for the large-scale of modern blast furnace, is a major milestone in the history of metallurgy.
2. Main Features of the Metallurgical Coke of COKE BREEZE 0-5mm:
• Quality assurance
• Mutual benefit
• Preferential price
3. Metallurgical Coke of COKE BREEZE 0-5mm Images:
4. Metallurgical Coke of COKE BREEZE 0-5mm Specification:
Parameters | Guarantee |
Moisture (ARB) | 5% max |
Ash (DB) | 12.50% max |
Volatile Matter (DB) | 1.4% max |
Sulphur (DB) | 0.7% max |
Phosphorus (DB) | 0.035% max |
CSR | 60% min |
CRI | 28% max |
M40 | 82% min |
M10 | 8% max |
Size 30-90 mm | 90% min |
+90 mm | 5% max |
-30mm | 5% max |
Mean Size | 52 mm |
5. FAQ
We have organized several common questions for our clients,may help you sincerely:
1) How to guarantee the quality of the products?
We have established the international advanced quality management system,every link from raw material to final product we have strict quality test;We resolutely put an end to unqualified products flowing into the market. At the same time, we will provide necessary follow-up service assurance.
2) What are coke's main physical properties?
The average heat capacity is 0.808 kj/(KGK) (100 ℃), 1.465 kj/(KGK) (1000 ℃)
Thermal conductivity is 2.64 kj/(MHK) (room temperature), 6.91 kj/(MHK) (900 ℃);
Ignition temperature (air) is 450-650 ℃.
3) How about your company?
Our company began to export coke when China cancelled 40% of coke export tariffs and quotas on January 1, 2013. We export many kinds of coke, such as CSR60 % and CSR 62% metallurgical coke (met coke), the NUT coke of 20 to 50 mm, coke breeze of 3 to 6 mm, and so on.
- Q: What is the density of coke?
- Do you want to transport by rail? Ha ha, you might as well ask the freight forwarding clerk, he / she will tell you the various models of the volume and the weight can be installed, the conversion of the density of the pile is more accurate.
- Q: Types of coke and use of coke
- Generally speaking, the use of coke in the following industries: blast furnace ironmaking, mechanical casting, calcium carbide production, processing Ferroalloy, chemical fertilizer, gas and high-tech high value-added industries
- Q: What is the difference between coking plant and coke plant
- Never heard of coke plant, coking plant is the production of coke products, there are other chemical products, it is estimated that you said the coke plant is the purchase of other people's desire to sell second-hand coke traders.
- Q: How coal is turned into coke in the coking chamber
- The kiln chamber wall set to continue burning, and some heat incoming kiln (indirect heating). High temperature gas flow (800 DEG C, is mixed with coal pyrolysis, chemical products into the fabric of unburned.
- Q: Some experimental results summarized the following two facts: the coke can not be used to restore aluminum mine, but it can be used for the reduction of copper and iron; no containing copper sulfate solution with tin, thus the activity sequence C, Al, Cu, Fe of the four elements is ______.
- K, Ca, Na, C, Mg, Al is not able to use C, CO, H2 and so on to restore the preparation of metal, because these metals are very active, can be used to restore copper and iron ore, indicating that the reduction of strong;
- Q: What are the requirements for coke and other accounts?
- 4, I personally set the password and password.5, the customer I own the bank transfer agreement, my ID card, bank debit card to the corresponding bank outlets for bank transfer procedures.6, the day of the day to accept the phone call Futures Company visit, after the successful return of T+1 days of commodity futures trading.7, the customer into the gold (silver period transfer; non bank transfer).8, customer online transactions (start trading).
- Q: What is the use of coke
- The physical properties of the coke coke coke screening composition, physical properties including bulk density, coke coke coke true relative density, apparent relative density and porosity of coke, coke, coke, thermal conductivity and specific heat of coke thermal stress, ignition temperature of coke, coke, coke thermal expansion coefficient of shrinkage, resistivity and permeability of coke coke. The physical properties of coke are closely related to its mechanical strength, thermal strength and chemical properties at room temperature. Following the main physical properties of coke: true density is 1.8-1.95g/cm3 0.88-1.08g/ cm3; apparent density; porosity is 35-55%; bulk density is 400-500kg/ m3; the average heat capacity is 0.808kj/ (KGK) (100 C), 1.465kj/ (KGK) (1000 DEG C); the thermal conductivity is 2.64kj/ (MHK) (room temperature), 6.91kg/ (MHK) (900 DEG C); ignition temperature (air) is 450-650 DEG C; dry ash free calorific value is 30-32KJ/g;
- Q: The sulfur content of coal and coke in general, the coking process of sulfur content of coal into the output of sulfur content of coke compared to those who are high and low?
- The sulfur content of coking coal basically all into the coke, only a small number into the gas but the number is very limited. How much coal is the amount of sulfur in the general coal is the sulfur. It should be said that coke is basically a little lower and a little bit limited.In the process of coking volatile will be a lot of consumption, ash will increase 2-3%.
- Q: What are the quality indicators of coke
- 2, the phosphorus in the coke: iron metallurgical coke coke content should be in the following 0.02 - 0.03%. 3, the ash content of coke: Coke Ash on the impact of the blast furnace smelting is very significant. Coke ash increased by 1%, coke consumption increased by 2 - 2.5%, therefore, the reduction of coke ash is very necessary. 4, volatile in coke: according to the volatile content of coke can determine the maturity of coke. Such as volatile content is greater than 1.5%, is said to produce coke; volatile less than 0.5 - 0.7%, it is said to be overdone, the general maturity of metallurgical coke volatile is divided into about 1%. 5, the moisture in the coke: water fluctuations will make the measurement of coke is not allowed, resulting in fluctuations in furnace conditions. In addition, the increase in the moisture content of Coke will make the M04 high, M10 is low, the drum index error. 6, the screening of coke composition: in the blast furnace coke particle size is also very important. In the past, the particle size of coke in our country is as follows: the coke size of large coke oven (1300 - 2000 square meters) is greater than 40 mm; the coke size of medium and small blast furnace is larger than 25 mm. However, some of the steel test shows that the coke particle size of 40 - 25 mm as well. Larger than 80 mm of coke to be whole, so that the particle size range. The coke block is uniform, the gap is large, the resistance is small, and the furnace condition runs well. Coke use: Shanxi sales all kinds of specifications of foundry coke, metallurgical coke, high sulfur coke trucks or wagons can transport
- Q: Mechanism of carbon and coke is not the same as the price which high?
- I am on the Ba Chau facility in Hebei during May this year, but now has more than 3 months, only 2 tons of carbon, and are defective pile to nobody in my barn. I bought a big machine, according to them is made of bark can make the raw material drying, but home. It's not going to work. I had to switch to coal drying, coal can not over drying, rework is often the case. Carefully down a do tons of carbon coal money to spend more than and 300. The great machine can not work normally, the basic propeller around 4 hours repair time, until now I have changed my sleeve 7
Send your message to us
Metallurgical Coke of COKE BREEZE 0-5mm
- Loading Port:
- Tianjin
- Payment Terms:
- TT OR LC
- Min Order Qty:
- 1000 m.t.
- Supply Capability:
- 1000000 m.t./month
OKorder Service Pledge
OKorder Financial Service
Similar products
Hot products
Hot Searches