1. Structure of Metallurgical Coke of Met coke of CRI 30 Description:
Sulfur content in coke: sulfur is one of the harmful impurities of iron smelting, it lower the quality of cast iron.The sulfur content in pig iron for steel making is more than 0.07% for the trash.By the blast furnace burden into furnace sulfur 11% came from the ore;3.5% from limestone;82.5% from coke, so coke is the main source of sulfur in charge.Coke sulfur content directly affect the blast furnace ironmaking production.When coke sulfur content is greater than 1.6%, sulfur, every 0.1% increase in coke consumption increased by 1.8%, increased by 3.7%, for the amount of limestone ore content of 0.3% by 1.5 - a 0.3% increase in the blast furnace production. The sulfur content of metallurgical coke is not greater than 1%, large and medium blast furnace using the sulphur content in metallurgical coke is less than 0.4-0.7%.
On China's coke production distribution, the regional distribution imbalance of coking enterprises, mainly distributed in north China, east China and northeast China.
2. Main Features of the Metallurgical Coke of Met coke of CRI 30:
• Quality assurance
• Mutual benefit
• Preferential price
• Various choice
3. Metallurgical Coke of Met coke of CRI 30 Images:
4. Metallurgical Coke of Met coke of CRI 30 Specification:
Parameters | Guarantee | Rejection |
Total Moisture (As received basis) | 5% max | |
Ash (dry basis) | 12.5% max | > 13.5% |
Volatile Matter (dry basis) | 1.5% max | > 1.8% |
Sulphur (dry basis) | 0.65% max | > 0.75% |
Phosphorus (dry basis) | 0.035% max | > 0.045% |
M10 | 7% max | > 9% |
M40 | 84% min | <82% |
CSR | 64% min | <62% |
CRI | 26% max | > 28% |
Size 30-90 mm | 90% min | |
+90 mm | 5% max | > 8% |
-30mm | 5% max | > 8% |
5. FAQ
The coke of phosphorus points: metallurgical coke ironmaking use phosphorus content should be below 0.02-0.03%.
- Q: What are the companies that produce coke
- Too many enterprises to produce coke. You search on Baidu, coke, a lot of business
- Q: What does Coke test index M25 mean?
- The index of pore structure is mainly expressed by the porosity rate (the percentage of the total volume of coke), which affects the reactivity and strength of coke. Different uses of different coke porosity index requirements, the general requirements of metallurgical coke porosity in the 40 ~ 45%, 35 ~ 40% in coke, coke export demand in about 30%. Coke crack degree and the porosity level, and the coking coal has a direct relationship, such as coal based coke refining, crack, high porosity, low strength; with coal as the foundation of the coal refining coke crack less, low porosity and high strength. The strength of coke is usually represented by two indices of crushing strength and abrasion resistance
- Q: Coke indicators are divided into grades
- Coke is a solid product of high temperature carbonization, the main component is carbon, is a crack and irregular pore structure (or porous). The number of cracks has a direct impact on the strength and crushing strength of the coke, the index is generally measured in terms of crack degree (the number of cracks in the unit volume coke).
- Q: How much coal can a kilogram of coal weigh?
- The ratio is about 1 to about 0.7, that is, about 1 kilograms of coking coal can produce a total of about 0.7 kg of coke
- Q: What is the essential difference between coal and coke?
- [coal]Coal is a kind of solid combustible mineral which is buried in the underground plants and has been formed by the complex biochemical and physicochemical changes. Coal is a kind of solid combustible organic rock, which is mainly formed by the chemical reaction of the remains of plants.
- Q: What are the requirements for the quality of coke in blast furnace smelting
- 4, volatile in coke: according to the volatile content of coke can determine the maturity of coke. Such as volatile content is greater than 1.5%, is said to produce coke; volatile less than 0.5 - 0.7%, it is said to be overdone, the general maturity of metallurgical coke volatile is divided into about 1%.5, the moisture in the coke: water fluctuations will make the measurement of coke is not allowed, resulting in fluctuations in furnace conditions. In addition, the increase in the moisture content of Coke will make the M04 high, M10 is low, the drum index error.6, the screening of coke composition: in the blast furnace coke particle size is also very important. In the past, the particle size of coke in our country is as follows: the coke size of large coke oven (1300 - 2000 square meters) is greater than 40 mm; the coke size of medium and small blast furnace is larger than 25 mm. However, some of the steel test shows that the coke particle size of 40 - 25 mm as well. Larger than 80 mm of coke to be whole, so that the particle size range. The coke block is uniform, the gap is large, the resistance is small, and the furnace condition runs well.
- Q: Do not understand why some of the indicators of coke is the cause of the full analysis of phosphorus or foundry use of this time?It is best to use the foundry requirements? Thank you
- Phosphorus is a kind of harmful element in metal, which reduces the mechanical properties of castings. Under normal circumstances, GB castings of phosphorus content requirements of less than 0.06%, the lower the special requirements
- Q: What is coke and how is coke classified?
- Metallurgical coke is coke, coke, iron alloy coke and non-ferrous metal smelting coke for metallurgical coke collectively. More than 90% are used in blast furnace, the furnace coke often called metallurgical coke. Metallurgical coke quality standard Chinese formulation (GB/T1996-94) is the blast furnace quality standards.Gasification coke is a kind of coke, which is specially used in the production of gas. It is mainly used in the fixed bed gas producer with solid slag, as the raw material to produce CO and H2 gas:C+O2 - CO2+408177KJCO2+C - 2CO-162142KJC+H2O - CO+H2-118628KJC+2H2O - CO2+2H2-75115KJBecause the process of producing the CO and H2 are endothermic reaction, need heat supplied by the coke combustion, so the heat is gasified char gasification process. The gasification coke required low ash content, high ash fusion point, block degree appropriate and uniform. The general requirements are as follows: >80% fixed carbon ash; 1250 degrees Celsius; volatile 84%, ash
- Q: What is coke? What is the use?
- Lay the foundation for large-scale modern blast furnace, is an important milepost in the history of metallurgy. The blast furnace operation and achieve good technical and economic indexes, smelting with coke (coke) must have appropriate chemical and physical properties, including thermal properties in the smelting process.
- Q: What's the difference between coke and coke?
- Higher than 550 DEG C, semi coke continues to decompose, precipitation of the remaining volatiles (the main component is hydrogen), semi coke weight loss at the same time contraction, the formation of cracks; temperature above the temperature of 800 degrees, the volume of semi coke hardens to form porous coke!
Send your message to us
Met coke of CRI 30
- Loading Port:
- Tianjin
- Payment Terms:
- TT OR LC
- Min Order Qty:
- 1000 m.t.
- Supply Capability:
- 100000 m.t./month
OKorder Service Pledge
OKorder Financial Service
Similar products
Hot products
Hot Searches
Related keywords