1. Structure of Metallurgical Coke of Coke Strength after Reactivity 60 Description:
Coke is made by high temperature metallurgical coke for blast furnace smelting, casting and gasification. Occurring in the process of coking after recovery and purification of coke oven gas is a high calorific value of fuel, is an important industrial raw material in organic synthesis.
Coke is mainly used for blast furnace ironmaking and used for copper, lead, zinc, titanium, antimony, mercury and other non-ferrous metal smelting of blast furnace, reducing agent, compound and the function of stock column frame.
Blast furnace with Coke instead of charcoal, which laid a foundation for the large-scale of modern blast furnace, is a major milestone in the history of metallurgy.
2. Main Features of the Metallurgical Coke of Coke Strength after Reactivity 60:
• Quality assurance
• Mutual benefit
• Preferential price
3. Metallurgical Coke of Coke Strength after Reactivity 60 Images:
4. Metallurgical Coke of Coke Strength after Reactivity 60 Specification:
Parameters | Guarantee |
Moisture (ARB) | 5% max |
Ash (DB) | 12.50% max |
Volatile Matter (DB) | 1.4% max |
Sulphur (DB) | 0.7% max |
Phosphorus (DB) | 0.035% max |
CSR | 60% min |
CRI | 28% max |
M40 | 82% min |
M10 | 8% max |
Size 30-90 mm | 90% min |
+90 mm | 5% max |
-30mm | 5% max |
Mean Size | 52 mm |
5. FAQ
We have organized several common questions for our clients,may help you sincerely:
1) How to guarantee the quality of the products?
We have established the international advanced quality management system,every link from raw material to final product we have strict quality test;We resolutely put an end to unqualified products flowing into the market. At the same time, we will provide necessary follow-up service assurance.
2) What are coke's main physical properties?
The average heat capacity is 0.808 kj/(KGK) (100 ℃), 1.465 kj/(KGK) (1000 ℃)
Thermal conductivity is 2.64 kj/(MHK) (room temperature), 6.91 kj/(MHK) (900 ℃);
Ignition temperature (air) is 450-650 ℃.
3) How about your company?
Our company began to export coke when China cancelled 40% of coke export tariffs and quotas on January 1, 2013. We export many kinds of coke, such as CSR60 % and CSR 62% metallurgical coke (met coke), the NUT coke of 20 to 50 mm, coke breeze of 3 to 6 mm, and so on.
- Q: We would like to export a batch of coke, I would like to know what information is required for a permit
- 2013 coke export tariffs and quota system has been canceled, with foreign trade business qualifications can be engaged in foreign trade coke business. After signing the coke export contract with the foreign trade, the foreign trade enterprise needs to apply for the electronic key to apply for the export license. The electronic key and export license shall be handled as follows:
- Q: Said the details can add points ah
- Visible: the two are called coke crushing strength index, has a certain correlation. Coking coking coal coke, the two general values are relatively large, and vice versa.The specific number of relations, to specific measurement of different manufacturers of coke M40 and M25 values, statistical regression, in order to determine.
- Q: Coke is divided into several kinds of specifications ah
- Use:Fixed carbon above 83; sulfur below 0.5; volatile below 1.5; about 15 ash coke for metallurgical e: mechanism: {; applied to steel coke particle size 8cm-150cm:{} with hot metal; for motor shell, radiator, mechanical counterweight cast char: {of} fertilizer for hot metal; coke bulk modified casting shell, radiator, electric}: {mechanical counterweight for ordinary casting furnace;} machinery parts and other parts suitable for roughly 2-3.5 tons of coke particle size for 25cm:{type common casting and casting products slightly strict; such as fire pump pipe fastener} fixed carbon above 85; volatile ash 13.5 1.5.; the following: 0.5; sulfur with coke particle size above 8cm for ordinary casting: {} 25cm {type coke particle size; for precision casting and ductile casting improved coke}:
- Q: China's coke iron smelting began in what time?
- Han also invented the "fried steel law", that is, the use of pig iron "fried" mature iron or steel of the new process, the product is called steel. At the same time, the rise of "100 steelmaking" technology. The Eastern Han Dynasty (AD 25 ~ 220), when the emperor of the Ming Dynasty, invented the hydraulic blast furnace, that is, "water discharge". The invention of ancient water row in China, about 1100 years earlier than europe. After the Han Dynasty, the method of steel. "Qi Shu Qi, even referred to as" places "big steel", later known as the filling steel, also known as steel group. This is another important achievement of the ancient steelmaking technology in china. According to the "Encyclopedia of" records: Chinese is the earliest use of coal iron country, the Han Dynasty have been tried, song and Yuan dynasties have been popularized. To the Ming Dynasty (AD 1368 ~ 1644) has been able to use coke smelting pig iron.
- Q: Who knows the proportion of pig iron and coke used in Cupola
- There are doubts: blank parts output is too low.3, blank export rate: raw materials into melting after the formation of blank, under normal circumstances, the common casting investment for every 1 tons of pig iron, scrap steel and other major raw materials, the lowest to 85% iron, after casting output blanks, nozzle, nozzle, riser, riser for iron smelting water ratio of about 30%; blank standard export rate, nozzle, riser re melted continue after put into use; production enterprises invested 1 tons per dryer, iron scrap and other major raw materials to the lowest 85% of the hot metal, roughly the same with ordinary casting, casting blank after the (standard yield) for hot metal ratio is about 70%, water riser for hot metal ratio is about 15%, and the same outlet riser re melted after continued use.
- Q: What is the phosphorus content in coke
- Generally, the phosphorus content of coke is low, about 0.02%.The bituminous coal is heated to 950-1050 DEG C under the condition of air isolation
- Q: What are the requirements for coke and other accounts?
- Coke futures margin is about 10% or so is quoted at $1169 per ton, trading units of 100 tons per hand, so do a coke about $11690.
- Q: How to remove the bottom of coke steel
- Finally, wash the rice cooker, stove, as well as your tired hands, thoroughly washed several times. Here, everything is back to normal, as if nothing had happened.After such a toss, the coke pot was removed, but the bottom layer of the so-called "nonstick layer" are often the early damage (normally always destroyed), it is impossible to. It's like trying to get rid of terrorists.If the bottom of the layer of carbon black is not easy to erase, even if, even with good. Some people may worry about eating into the carbon poisoning, I think there is no need to worry about this. Wenchuan earthquake hero, Mr. Zhu Jianqiang, light to eat charcoal for 36 days, you can see the toxicity of carbon nothing. Moreover, after cleaning the rice cooker in the layer of carbon black has very little
- Q: The sulfur content of coal and coke in general, the coking process of sulfur content of coal into the output of sulfur content of coke compared to those who are high and low?
- The sulfur content of coking coal basically all into the coke, only a small number into the gas but the number is very limited. How much coal is the amount of sulfur in the general coal is the sulfur. It should be said that coke is basically a little lower and a little bit limited.In the process of coking volatile will be a lot of consumption, ash will increase 2-3%.
- Q: What is the difference between coke and semi coke in ferrosilicon smelting process? In the process of energy statistics in the end should be 0.9714 of the conversion coefficient should be used with the conversion coefficient of 0.75 x 0.9714, please expert advice? emergencyUrgent!
- Coke is used for smelting iron alloy coke, and the coke is used in blast furnace and used for copper, lead, zinc, titanium, antimony, mercury and other non-ferrous metal smelting of blast furnace, reducing agent, heating agent and columnar skeleton.
Send your message to us
Metallurgical Coke of Coke Strength after reactivity 60
- Loading Port:
- Tianjin
- Payment Terms:
- TT or LC
- Min Order Qty:
- 1000 m.t.
- Supply Capability:
- 1000000 m.t./month
OKorder Service Pledge
OKorder Financial Service
Similar products
Hot products
Hot Searches