• CNBM  Nut        Coke   with   Normal   Phosphorous System 1
  • CNBM  Nut        Coke   with   Normal   Phosphorous System 2
  • CNBM  Nut        Coke   with   Normal   Phosphorous System 3
  • CNBM  Nut        Coke   with   Normal   Phosphorous System 4
CNBM  Nut        Coke   with   Normal   Phosphorous

CNBM Nut Coke with Normal Phosphorous

Ref Price:
get latest price
Loading Port:
Tianjin
Payment Terms:
TT OR LC
Min Order Qty:
100 m.t.
Supply Capability:
3000 m.t./month

Add to My Favorites

Follow us:


OKorder Service Pledge

Quality Product, Order Online Tracking, Timely Delivery

OKorder Financial Service

Credit Rating, Credit Services, Credit Purchasing

1. Structure of Nut   Coke   with   Normal   Phosphorous Description

Coke is made by high temperature metallurgical coke for blast furnace smelting, casting and gasification. Occurring in the process of coking after recovery and purification of coke oven gas is a high calorific value of fuel, is an important industrial raw material in organic synthesis.

Coke is mainly used for blast furnace ironmaking and used for copper, lead, zinc, titanium, antimony, mercury and other non-ferrous metal smelting of blast furnace, reducing agent, compound and the function of stock column frame.

Blast furnace with Coke instead of charcoal, which laid a foundation for the large-scale of modern blast furnace, is a major milestone in the history of metallurgy.

2. Main Features of the Nut   Coke   with   Normal   Phosphorous

     Quality assurance

     Mutual benefit

     Preferential price

     Various choice

3. Nut   Coke   with   Normal   Phosphorous Images:

 

CNBM  Nut        Coke   with   Normal   Phosphorous

CNBM  Nut        Coke   with   Normal   Phosphorous

CNBM  Nut        Coke   with   Normal   Phosphorous

CNBM  Nut        Coke   with   Normal   Phosphorous


4. Nut   Coke   with   Normal   Phosphorous Specification:

 

Parameters

Guarantee

Rejection

Total Moisture ( As received basis )

8% max


Ash ( dry basis )

12.5% max

> 13.5%

Volatile   Matter ( dry   basis )

1.5% max

> 1.8%

Sulphur ( dry basis )

0.70% max

> 0.80%

Phosphorus ( dry basis )

0.035% max

> 0.045%

Size 10-30 mm

90% min


+30 mm

5% max

> 8%

-10 mm

5% max

>8%


5. FAQ

We have organized several common questions for our clients,may help you sincerely:

1) How to guarantee the quality of the products

We have established the international advanced quality management system,every link from raw material to final product we have strict quality test;We resolutely put an end to unqualified products flowing into the market. At the same time, we will provide necessary follow-up service assurance.

2) What are coke's main physical properties?

The average heat capacity is 0.808 kj/(KGK) (100 ℃), 1.465 kj/(KGK) (1000 ℃)

Thermal conductivity is 2.64 kj/(MHK) (room temperature), 6.91 kj/(MHK) (900 ℃);

Ignition temperature (air) is 450-650 ℃.

3) How about your company

Our company began to export coke when China cancelled 40% of coke export tariffs and quotas on January 1, 2013. We export many kinds of coke, such as CSR60 % and CSR 62% metallurgical coke (met coke), the NUT coke of 20 to 50 mm, coke breeze of 3 to 6 mm, and so on.


Q: Said the details can add points ah
Both are expressed in terms of the crushing strength of the cold mechanical strength index of coke quality.Among them, because of the specific measurement methods are not the same, so the use of different records.
Q: Why is coke used in blast furnace steelmaking?Why not use coal?
The role of coke in blast furnace steelmaking is as follows:(1) providing heat: the coke burns fiercely in the raceway in front of the tuyere of the coke oven, and the heat generated by the combustion is the main heat source in the process of blast furnace smelting.
Q: What is the amount of waste gas produced by a ton of coke burning
The coking coal is heated to 1000 DEG C under the condition of isolated air (high temperature carbonization)
Q: What is the essential difference between coal and coke?
(1) power coal(2) coking coal (bituminous coal)(3) coal used in coal chemical industry, which mainly includes gasification coal, coal for low temperature carbonization, hydrogenation of liquefied coal and so on.
Q: The chemical composition of coke m10.m25 refers to?
1, coal washing ((M25 drum index) metallurgical coke crushing strength is (M10 drum index) metallurgical coke wear strength is reflected
Q: Do not understand why some of the indicators of coke is the cause of the full analysis of phosphorus or foundry use of this time?It is best to use the foundry requirements? Thank you
As everyone knows, sulfur and phosphorus is harmful substances in the metal, because the sulfur is out in coke processing, so this index is not required, but the phosphorus in this process has not been effectively removed, so this is the requirement of foundry process or smelting plant. Phosphorus can reduce the strength of the metal, will lead to the metal "cold crisp", so to control the phosphorus content of coke, to prevent phosphorus into the metal.
Q: What does the M40% and M25% mean in the analysis of coke?
(1) crushing strength (shatter strength): the ability of a certain particle size coal sample to fall under the condition of free fall.
Q: What are the quality indicators of coke
Coke is a solid product of high temperature carbonization, the main component is carbon, is a crack and irregular pore structure (or porous). The number of cracks has a direct impact on the strength and crushing strength of the coke, the index is generally measured in terms of crack degree (the number of cracks in the unit volume coke). The index of pore structure is mainly expressed by the porosity rate (the percentage of the total volume of coke), which affects the reactivity and strength of coke.
Q: What is the effect of coke moisture on the blast furnace?
The influence of coke moisture on blast furnace can be divided into two parts:
Q: Mechanism of carbon and coke is not the same as the price which high?
I am on the Ba Chau facility in Hebei during May this year, but now has more than 3 months, only 2 tons of carbon, and are defective pile to nobody in my barn. I bought a big machine, according to them is made of bark can make the raw material drying, but home. It's not going to work. I had to switch to coal drying, coal can not over drying, rework is often the case. Carefully down a do tons of carbon coal money to spend more than and 300. The great machine can not work normally, the basic propeller around 4 hours repair time, until now I have changed my sleeve 7

Send your message to us

This is not what you are looking for? Post Buying Request

Similar products

Hot products


Hot Searches

Related keywords