• The   Metallurgical   Coke   of   Size   is   30   –   90   mm System 1
  • The   Metallurgical   Coke   of   Size   is   30   –   90   mm System 2
  • The   Metallurgical   Coke   of   Size   is   30   –   90   mm System 3
The   Metallurgical   Coke   of   Size   is   30   –   90   mm

The Metallurgical Coke of Size is 30 – 90 mm

Ref Price:
get latest price
Loading Port:
Tianjin
Payment Terms:
TT OR LC
Min Order Qty:
100 m.t.
Supply Capability:
3000 m.t./month

Add to My Favorites

Follow us:


OKorder Service Pledge

Quality Product, Order Online Tracking, Timely Delivery

OKorder Financial Service

Credit Rating, Credit Services, Credit Purchasing

1. Structure of The Metallurgical Coke of Size is 30 – 90 mm Description

Coke is made by high temperature metallurgical coke for blast furnace smelting, casting and gasification. Occurring in the process of coking after recovery and purification of coke oven gas is a high calorific value of fuel, is an important industrial raw material in organic synthesis.

Coke is mainly used for blast furnace ironmaking and used for copper, lead, zinc, titanium, antimony, mercury and other non-ferrous metal smelting of blast furnace, reducing agent, compound and the function of stock column frame.

Blast furnace with Coke instead of charcoal, which laid a foundation for the large-scale of modern blast furnace, is a major milestone in the history of metallurgy.

2. Main Features of The Metallurgical Coke of Size is 30 – 90 mm

     Quality assurance

     Mutual benefit

     Preferential price

     Various choice

3.The Metallurgical Coke of Size is 30 – 90 mm Images:

 


4.The Metallurgical Coke of Size is 30 – 90 mm Specification:

 

Parameters

Guarantee

Moisture (ARB)

5% max

Ash (DB)

12.50% max

Volatile Matter (DB)

1.5% max

Sulphur (DB)

0.65% max

Phosphorus (DB)

0.035% max

CSR

66% min

CRI

28% max

M40

82% min

M10

8% max

Size 30-90 mm

90% min

+90 mm

5% max

-30mm

5% max


5. FAQ

We have organized several common questions for our clients,may help you sincerely:

1) How to guarantee the quality of the products

We have established the international advanced quality management system,every link from raw material to final product we have strict quality test;We resolutely put an end to unqualified products flowing into the market. At the same time, we will provide necessary follow-up service assurance.

2) What are coke's main physical properties?

The average heat capacity is 0.808 kj/(KGK) (100 ℃), 1.465 kj/(KGK) (1000 ℃)

Thermal conductivity is 2.64 kj/(MHK) (room temperature), 6.91 kj/(MHK) (900 ℃);

Ignition temperature (air) is 450-650 ℃.

3) How about your company

Our company began to export coke when China cancelled 40% of coke export tariffs and quotas on January 1, 2013. We export many kinds of coke, such as CSR60 % and CSR 62% metallurgical coke (met coke), the NUT coke of 20 to 50 mm, coke breeze of 3 to 6 mm, and so on.


Q: Coke is how to produce, what is its purpose?
Under the condition of air isolation, the bituminous coal is heated to 950-1050 DEG C, which is finally made into coke by drying, pyrolysis, melting, bonding, solidification and shrinkage. Coke oven gas produced in the process of coking and recovery is not only a high calorific value of fuel, but also an important industrial raw material for organic synthesis.
Q: What does Coke test index M25 mean?
The index of pore structure is mainly expressed by the porosity rate (the percentage of the total volume of coke), which affects the reactivity and strength of coke. Different uses of different coke porosity index requirements, the general requirements of metallurgical coke porosity in the 40 ~ 45%, 35 ~ 40% in coke, coke export demand in about 30%. Coke crack degree and the porosity level, and the coking coal has a direct relationship, such as coal based coke refining, crack, high porosity, low strength; with coal as the foundation of the coal refining coke crack less, low porosity and high strength. The strength of coke is usually represented by two indices of crushing strength and abrasion resistance
Q: We would like to export a batch of coke, I would like to know what information is required for a permit
2013 coke export tariffs and quota system has been canceled, with foreign trade business qualifications can be engaged in foreign trade coke business. After signing the coke export contract with the foreign trade, the foreign trade enterprise needs to apply for the electronic key to apply for the export license. The electronic key and export license shall be handled as follows:
Q: Used in a restaurant?Dry or dry carbon carbon, coke or coke, and I do not know which word is a word of this sound. The use of coke for iron making. They are more than 1000 yuan price.The main problem is: dry carbon is coke?Toxic smoke, then the chimney can not do? Can I use the blower?
Metallurgical coke is coke, coke, iron alloy coke and non-ferrous metal smelting coke ". Since more than 90% of metallurgical coke is used for blast furnace ironmaking, it is often referred to as coke.
Q: After the long-term use of non stick pan, oil stains can not be effectively removed, over a long period of time in the non stick coating on the formation of a layer of coke, the effect of losing non stick. As a result of this layer of coke is relatively dense and smooth, scouring cloth has been ineffective, steel ball can not be used to damage the coating, what chemical or physical methods to remove this layer of coke?
After such a toss, the coke pot was removed, but the bottom layer of the so-called "nonstick layer" are often the early damage (normally always destroyed), it is impossible to. It's like trying to get rid of terrorists.If the bottom of the layer of carbon black is not easy to erase, even if, even with good. Some people may worry about eating into the carbon poisoning, I think there is no need to worry about this. Wenchuan earthquake hero, Mr. Zhu Jianqiang, light to eat charcoal for 36 days, you can see the toxicity of carbon nothing. Moreover, after cleaning the rice cooker in the layer of carbon black has very little
Q: I now do a good job in the coke network editor, I would like to know more about coke
(2) reducing agent.The reduction of ore in blast furnace is accomplished by indirect reduction and direct reduction. The indirect reduction is about 400 degrees centigrade. The indirect reduction is rising gas CO reduction in ore, iron oxide from high iron gradually reduced low iron until the metal iron, while producing CO2:
Q: Natural gas can replace coke smelting pig iron
Coke at high temperature (also some blast furnace pulverized coal, heavy oil, natural gas and other auxiliary fuel) in carbon with bubbling air oxygen in the combustion of carbon monoxide and hydrogen generated in the furnace, removing the rise in iron ore in the process of oxygen, thereby reducing iron. The molten iron is released from the taphole. An iron ore, which is a mixture of non - reducing impurities, such as limestone, to form a slag from the slag. The produced gas is discharged from the top of the furnace, and is used as a fuel for a hot blast stove, a heating furnace, a coke oven, a boiler, etc.. Blast furnace smelting is the main product of pig iron, as well as by-products of blast furnace slag and blast furnace gas.
Q: What is coke and how is coke classified?
Types of cokeCoke is usually divided by use of metallurgical coke (including blast furnace coke, coke and iron alloy coke, calcium carbide and coke gasification etc.) with coke. The pressurized pulverized coal forming coal, coke carbonization etc. in the new postprocessing process called Formcoke.
Q: Effect of coke powder ratio on the index
2, the phosphorus content of coke: iron metallurgical coke content should be 0.02 - 0.03%.3, coke ash: blast furnace coke ash effect is very significant. The amount of coke ash in coke increased by 1%, an increase of 2 - 2.5%., therefore, a decrease in coke ash is necessary4, coke volatile: according to the coke can be judged by the volatile content of volatile volatile is greater than 1.5%, then the coke; volatile less than 0.5 - 0.7%, which means that too much, generally mature volatile metallurgical coke to about 1%.5, coke moisture: moisture fluctuations should not be measured in coke, causing fluctuations in the furnace conditions. In addition, increased M04 coke moisture content high, low M10, the drum index error
Q: What is the difference between coke and coking coal
Coking coal is a kind of bituminous coal with a high degree of deterioration, and the thermal stability of the resultant colloid is good when the coke is produced separately. The block size of the coke is large, the crack is small and the strength is high

Send your message to us

This is not what you are looking for? Post Buying Request

Similar products

Hot products


Hot Searches