Metallurgical Coke of Coke Strength after Reactivity 65
- Loading Port:
- Tianjin
- Payment Terms:
- TT OR LC
- Min Order Qty:
- 100 m.t.
- Supply Capability:
- 3000 m.t./month
OKorder Service Pledge
OKorder Financial Service
You Might Also Like
1. Structure of Metallurgical Coke of Coke Strength after Reactivity 65 Description:
Coke is made by high temperature metallurgical coke for blast furnace smelting, casting and gasification. Occurring in the process of coking after recovery and purification of coke oven gas is a high calorific value of fuel, is an important industrial raw material in organic synthesis.
Coke is mainly used for blast furnace ironmaking and used for copper, lead, zinc, titanium, antimony, mercury and other non-ferrous metal smelting of blast furnace, reducing agent, compound and the function of stock column frame.
Blast furnace with Coke instead of charcoal, which laid a foundation for the large-scale of modern blast furnace, is a major milestone in the history of metallurgy.
2. Main Features of the Metallurgical Coke of Coke Strength after Reactivity 65:
• Quality assurance
• Mutual benefit
• Preferential price
• Various choice
3. Metallurgical Coke of Coke Strength after Reactivity 65 Images:
4. Metallurgical Coke of Coke Strength after Reactivity 65 Specification:
Parameters | Guarantee |
Moisture (ARB) | 5% max |
Ash (DB) | 12.50% max |
Volatile Matter (DB) | 1.5% max |
Sulphur (DB) | 0.65% max |
Phosphorus (DB) | 0.035% max |
CSR | 66% min |
CRI | 28% max |
M40 | 82% min |
M10 | 8% max |
Size 30-90 mm | 90% min |
+90 mm | 5% max |
-30mm | 5% max |
5. FAQ
We have organized several common questions for our clients,may help you sincerely:
1) How to guarantee the quality of the products?
We have established the international advanced quality management system,every link from raw material to final product we have strict quality test;We resolutely put an end to unqualified products flowing into the market. At the same time, we will provide necessary follow-up service assurance.
2) What are coke's main physical properties?
The average heat capacity is 0.808 kj/(KGK) (100 ℃), 1.465 kj/(KGK) (1000 ℃)
Thermal conductivity is 2.64 kj/(MHK) (room temperature), 6.91 kj/(MHK) (900 ℃);
Ignition temperature (air) is 450-650 ℃.
3) How about your company?
Our company began to export coke when China cancelled 40% of coke export tariffs and quotas on January 1, 2013. We export many kinds of coke, such as CSR60 % and CSR 62% metallurgical coke (met coke), the NUT coke of 20 to 50 mm, coke breeze of 3 to 6 mm, and so on.
- Q: Standard grade two grade coke standard
- Evaluation of coke quality1, sulfur content in coke: sulfur is a harmful impurity of iron smelting, which reduce the quality of pig iron. The sulfur content in the pig iron is more than 0.07%. 11% of the sulfur from the blast furnace charge into the furnace comes from the ore, and the other comes from the limestone; the other is from the coke, so the coke is the main source of sulfur in the charge of the 82.5% of the charge. Sulfur content in coke directly affects the production of blast furnace. When the sulfur content in coke is greater than 1.6%, sulfur increased 0.1%, the amount of coke increased 1.8%, limestone amount increased 3.7%, 0.3% increase in amount of ore blast furnace output to reduce the sulfur content under 1.5 - 2.0%. metallurgical coke is not greater than 1%, the use of large and medium-sized metallurgical coke content in blast furnace is less than 0.4 - 0.7%.
- Q: What is the reasonable standard of volatile content of coke
- Generally speaking, the volatile content of coke is about 1.5 or so, but not more than 2
- Q: Said the details can add points ah
- Both are expressed in terms of the crushing strength of the cold mechanical strength index of coke quality.Among them, because of the specific measurement methods are not the same, so the use of different records.
- Q: Coke is divided into several kinds of specifications ah
- Use:Fixed carbon above 83; sulfur below 0.5; volatile below 1.5; about 15 ash coke for metallurgical e: mechanism: {; applied to steel coke particle size 8cm-150cm:{} with hot metal; for motor shell, radiator, mechanical counterweight cast char: {of} fertilizer for hot metal; coke bulk modified casting shell, radiator, electric}: {mechanical counterweight for ordinary casting furnace;} machinery parts and other parts suitable for roughly 2-3.5 tons of coke particle size for 25cm:{type common casting and casting products slightly strict; such as fire pump pipe fastener} fixed carbon above 85; volatile ash 13.5 1.5.; the following: 0.5; sulfur with coke particle size above 8cm for ordinary casting: {} 25cm {type coke particle size; for precision casting and ductile casting improved coke}:
- Q: Who knows the proportion of pig iron and coke used in Cupola
- There are doubts: if the scrap ratio is too large to increase the difficulty of processing, product quality can not be guaranteed. The proportion is too high or too low are abnormal.2, auxiliary material input: foundry auxiliary materials mainly coke. Ordinary casting (except dry cylinder) 1 tons ~ ~ 5 tons cupola, each investment of 1 tons of coke, according to the situation of the piece can be from 4.5 tons to 5.5 tons. Ordinary blank (special pieces extra), 5 tons to 10 tons per 1 tons of coke in cupola furnace about 6.5 tons to 7.5 tons of blank (waste products re melted are calculated according to the above method).
- Q: Some experimental results summarized the following two facts: the coke can not be used to restore aluminum mine, but it can be used for the reduction of copper and iron; no containing copper sulfate solution with tin, thus the activity sequence C, Al, Cu, Fe of the four elements is ______.
- There is no containing copper sulfate solution with tin. Because the copper iron can be displaced from the salt solution in their description, copper and iron;To sum up, we can know that C, Al, Cu, Fe four elements of the order of activity is Al > C > Fe > Cu;The answer is: Al > C > Fe > Cu.
- Q: Why is coke used in blast furnace steelmaking?Why not use coal?
- (2) reduction: high temperature gas generated in coke combustion in the raceway, passed to the material in the process of heat rising, the endothermic reaction and coke formation, CO and H2, then CO and iron oxide in iron ore reduction reaction is transformed into metallic iron.(3) the role of the skeleton: the blast furnace smelting process occurs in the movement and interaction between the rising of the gas and the falling of the charge. The pellets, coke, iron ore, ore and other materials according to a certain proportion, and batch sequence into a blast furnace, blast furnace smelting in reducing atmosphere under the hot metal, after providing to the steelmaking plant of the steel-making.
- Q: What is the phosphorus content in coke
- Coke obtained from high temperature coking for blast furnace smelting, casting and gasification. Coke oven gas produced in the process of coking and recovery is not only a high calorific value of fuel, but also an important industrial raw material for organic synthesis.
- Q: What is the effect of coke moisture on the blast furnace?
- 1, a large number of high coke moisture (when the rain open storage of coke in blast furnace smelting coke), if not timely load back down, will cause a relatively large impact on the furnace, coke is better then no timely adjusting load will cause heat phenomenon.
- Q: Distinction and distinction of cokeSoil coke, improved coke, coke machine coke do, what is the difference between
- 2, gasification coke, is dedicated to the production of coke gas, mainly used for solid slag in the fixed bed gas producer, as a gasification raw material, the production of CO and H2 as a combustible component of the gas:C+O2 - CO2+408177KJCO2+C - 2CO-162142KJC+H2O - CO+H2-118628KJC+2H2O - CO2+2H2-75115KJBecause the process of producing the CO and H2 are endothermic reaction, need heat supplied by the coke combustion, so the heat is gasified char gasification process. The gasification coke required low ash content, high ash fusion point, block proper and uniform.
Send your message to us
Metallurgical Coke of Coke Strength after Reactivity 65
- Loading Port:
- Tianjin
- Payment Terms:
- TT OR LC
- Min Order Qty:
- 100 m.t.
- Supply Capability:
- 3000 m.t./month
OKorder Service Pledge
OKorder Financial Service
Similar products
Hot products
Hot Searches