• AA5052 Aluminium wire for woven mesh product System 1
AA5052 Aluminium wire for woven mesh product

AA5052 Aluminium wire for woven mesh product

Ref Price:
get latest price
Loading Port:
Shanghai
Payment Terms:
TT or LC
Min Order Qty:
2 m.t.
Supply Capability:
20000 m.t./month

Add to My Favorites

Follow us:


OKorder Service Pledge

Quality Product, Order Online Tracking, Timely Delivery

OKorder Financial Service

Credit Rating, Credit Services, Credit Purchasing

1、 Structure of  Aluminium Wire Description

Soft aluminum wire  is made from prime material, 

The Aluminium wire has advantages over good anti-corrosiveness. well electrical

 conductivity and processiveness. And it also is a kind of best choice for color-match after anodic process.

 

2Main Features of the AA5052 Aluminium Wire

  (a) Good conductivity

(b) Directly soldering

(c) High ductility,good colorability

(d) Good chemically resistance

(e) Excellent thermal stability            

3 Aluminium Wire Images

 

4Aluminium Wire Specification

  

Product

Pure aluminum

Corrosionresisting aluminum alloy

Brand

YH-301

YH-331

YH-5356

YH-311

Standard and steel grade

GB

S301

S331

S5356

S311

AWS

ER1100

ER5183

ER5356

ER4043

Gauge Φ(mm)

0.8-5.0

0.8-5.0

0.8-5.0

0.8-5.0

Welding wire chemical composition(%)

Cu

0.05~0.20

≤0.10

≤0.10

≤0.30

Si

≤1.0

≤0.40

≤0.25

4.5~6.0

Fe

-

≤0.40

≤0.40

≤0.80

Mn

≤0.05

0.05~1.00

0.05~0.20

≤0.05

Mg

-

4.3~5.2

4.5~5.5

≤0.05

Cr

-

0.05~0.25

0.05~0.20

-

Zn

≤0.10

≤0.25

≤0.10

≤0.10

Ti

-

≤0.15

0.06-0.20

≤0.20

Al

≥99.5

Rem

Rem

Rem

 

5FAQ of  AA5052 Aluminium Wire

 a.What is monthly capacity

 ---CNBM is one stated own company and our monthly capacity is about  2000tons.

b. Now which countries do you export your goods?

----Now we export to  South East Asia,Africa, North America,South America  ect.

 

Q:Put the aluminum wire into the ferrous sulfate solution. What color changes on the surface of the aluminum wire?
Reason: ferric chloride hydrolysis is acidic, and hydrogen ions in solution react with metal aluminum
Q:Copper wire, wire, aluminum wire each, write out the characteristics of the three metals
Iron wire: wire is also conductive, but there is no copper wire, aluminum wire is good, usually used only to tie things;
Q:How can I change the fuse?
If it's the air switch, just switch the switch up. If not, it is better to replace the fuse into an air switch, so that it can be pulled out again after the trip.
Q:The air outlet of an aluminum screw into Skoda crystal sharp front windshield!
1, basically no impact on the car, instrument panel inside all wire harness, there are packaging, will not be broken.3, to 4S shop hours cost to hundreds of dollars
Q:What can drum up Water Leakage glue
The Water Leakage oil clean, dripping glue, glue can be used 502, good brothers (AB), best to use glass glue dry a long time.
Q:Aluminum wirMay not be related to the type of lubricant chosen.e through the mold, why not bright?
Suggest you use BW-500F aluminum acid degreasing agent, and BW-286 aluminum chrome free passivation agent collocation, the treatment of aluminum wire surface bright and form a layer of conductive passivation film, the effect is good.
Q:How to remove the wok of the grease and bottom ash
The washing powder or clean water into the pot after the first precise use of cloth dipped in water to wipe it again, after a while and then brushed aluminum. Iron pot of the group of imitation aluminum wire (such as electric wire like) eraser, stained with washing powder, water wipe, no oil pollution. Our kitchen has not been cleaned for 5 years, it's dirty, and we have many ways to do it. Finally, we use this method to clean the kitchen. It is as white as new. You can try it,
Q:How do you make the faucet HOSE?
Furthermore, adjust the pressure to take machine embossing mold elastic, put a head to the embossing (embossing hose is six cap and braided hose connection the stainless steel cap). Not too tight not too loose as copper core, embossing mold need to reset, just like the other end in embossing. The hose will be fine. It's only packed. Pointed hose (single hole, hot water hose) 40CM, 50CM, that's hard to say. It's entirely cut by the length of the pointed tooth. Pointed teeth have 28 heads, 32 heads, 38 heads, 42 heads and 100 heads. Others are the same as above
Q:How to bind overhead wires?
The main components of overhead lines are wires and lightning wires (overhead ground wires), towers, insulators, fittings, tower foundations, cables and earthing devices.
Q:Copper wire drawing machine with copper wire drawing machine, what is the difference
Drawing machine mechanical reduction rate is not the same, when the mechanical reduction rate of copper clad aluminum alloy wire drawing machine design is so the face should be smaller and the copper wire

1. Manufacturer Overview

Location
Year Established
Annual Output Value
Main Markets
Company Certifications

2. Manufacturer Certificates

a) Certification Name  
Range  
Reference  
Validity Period  

3. Manufacturer Capability

a)Trade Capacity  
Nearest Port
Export Percentage
No.of Employees in Trade Department
Language Spoken:
b)Factory Information  
Factory Size:
No. of Production Lines
Contract Manufacturing
Product Price Range

Send your message to us

This is not what you are looking for? Post Buying Request

Similar products

New products

Hot products


Hot Searches

Related keywords